The compressibility of Indium

Not many people realize that Indium is actually 4 times softer than lead. In this picture you can see that with just a standard vise I could compress this penny into a .004" thick piece of

Products

New TIM Web Site

Welcome to the new Indium Blog. We have Indium Thermal Team Members that will constantly be adding to this blog. They will include Bob Jarrett, Amanda Whittemore, Adrian Low, Jim Hisert and many

Support

Settling in at Woodstock

Folks, It has been 2 months now that I have lived in Woodstock, VT. Some interesting observations: 1. The church I attend, The First Congregational Church is pastored by Norman Koop, former Surgeon

Products

Join Me at CONCIBE 2007 in Guadalajara June 7th and 8th

Folks, I will be giving four, one hour workshops at CONCIBE 2007 in beautiful Guadalajara, Mexico on June 7th and 8th. A summary of the topics follows:

Archive

Happy Birthday, Helvetica!

It's gifts of gold as Helvetica celebrates it's 50th. Yes, that venerable font, Helvetica, has been with us since

Products

Counterfeit Components: A Big Threat to the Electronics Industry

Folks, I have written a soon to be published article, with Sea View Technologies colleague Phil Perry, for Circuitree magazine about the threat of counterfeit components. For me it was one of the

Products

Indium Corporation Wins Premiere Advertising Award

Indium Corporation has earned the prestigious Pro-Comm Award for the world's first electronics assembly materials online video advertisement. In addition to winning the award, the ad, titled

Products

Increasing Costs of Commodities Only a 2nd Order Effect on Electronics

Folks, There has recently been concern over the raising price of commodities (e.g.: copper, tin, silver, gold, cement, steel, oil, lumber, etc). So it is only natural to ask how it affects

Support

Dr. Ron posts 3rd Scientific American Article

Folks, As I believe I have shared before, one of my hobbies is understanding and esplaining physics concepts like the Theory of Relativity and Quantum Mechanics at a lay person level. Scientific

Products

Some Still Looking for RoHS to be Repealed

Folks, I recently received this note: Hello Dr. Ron, A colleague of mine sent me the following article. I’m about to start the Pb-Free implementation and wondering where do we stand. Regards,

Products

India not the Future China

Folks, Many people view India as the future China. While this is already true for help centers and telecommunications technology, for electronic assembly, India lacks several critical requirements.

Support

Interview with Dartmouth Grad and New Indium Employee Anny Zhang

Folks, One of my most successful graduate students at Dartmouth was Anny Zhang. She was a Masters in Engineering Management student and is curretly a new employee at Indium Corp. I thought readers

Archive

Thoughts on WEEE/RoHS Implementation

Folks, The EU is currently assessing the effect of WEEE/RoHS on industry. A recent article from EDN discusses this interesting topic. To no one's surprise the "paperwork" aspects of the

Archive

WOM: China Style

I am fortunate to be able to speak at social media events, and to attend others. For examples, I recently presented at theISBM'sannualmeeting in Tampa, Florida, and I am attending theWOMMAevent

Products

These Come From Trees … and vandals

It's one thing when a company establishes and controls their message to their audience. It's entirely another when a third-party takes over the company's store/product for another

Products

01005 Passives Not Really 01005 in Size

Folks, I mentioned this in the quiz at the left, but am I the only one that didn't know that a 01005 passive is really not that size? The designation 01005 means that the passive should be 0.010

Archive

New B2B Electronics Assembly Blog Launched

Future Fab Bloghas just been announced. According to their site,"it is written by the editorial panel members ofFuture Fab International. It's aim is to focus on the semiconductor,

Products

WEEE/RoHS Type Compliance Frustrating for Industry Leaders

Folks, A fellow WEEE/RoHS Warrior writes the following note and asks readers to share their thoughts and experiences. Cheers, Dr. Ron Dear Dr. Ron, After now having worked for a fairly large OEM for

Products

Another B2B Online Video Ad Released

We have just released the third in a series of online video ads aimed at our B2B electronics assembly audience. The series is titled: INDIUM CORPORATION: We Know SMT Inside & Out. This ad is

Products

The Miracle of Soldering

Folks, That soldering is a miracle there is no doubt. Just coincidentally, copper, the best practical conductor of electricity, can be bonded electrically and mechanically with solder at temperatures

Products

Dr Ning-Cheng Lee Discusses Chinese Lead Free Alloys

Folks, At APEX 2007 Indium Corp's Dr. Ning-Cheng Lee and I were interviewed by PCB007 Re China RoHS. Dr. Lee discussed the "Chinese" lead-free alloys that contain 0.03 to 0.05% Cerium.

At Indium we research, develop, and manufacture advanced electronics assembly materials solutions to the challenges of today, tomorrow, and the future.