Thermocompression Bonding for Microbump Flip-Chip Soldering

For reasons that I will discuss in a post later this year, a common factor that is emerging in the area of copper-pillar microbump 2.5D and 3D joining, is the adoption of thermocompression (TC)

Products

Indium Wire and Cryogenic Sealing

Indium wire is ideal for many sealing applications, especially cryogenic

Products

Solder Alloy Densities: Comparing Calculated to Actual

Folks, I have occasionally written on calculating solder alloy density, as there is surprisingly more interest than I thought there would be in this

Products

Alternate Lead-Free Tabbing Alloys for Solar Module Assembly

Today I received an interesting email that could be useful for my readers. Here goes: “Dear Jim, I saw your recent blog. I am in the process of prototyping a photovoltaic application. I am

Products

Indium Solar: A New Booth Location at Intersolar 2011

On behalf of our solar PV team here at Indium Corporation, I’d like to mention how excited we are to see you at Intersolar in

Support

The Power of the Universe

In the last few months, it seems I have been often reminded how powerful the universe can be.Today, checking my email, I found some fantastical photos of Puyehue volcano, in Chile, erupting.This

Products

SMT Reflow Process Window: Solder Paste Maximum Slope vs. Ramp (or Average) Rate

Included in a solder paste‘s Product Data Sheet, among other things, are general guidelines which aid the customer in designing an SMT reflow profile. The data sheet gives general

Products

Flux Evaluation for AuSn High Temperature Solder Reflow

Recent test results show that solder fluxes handle high reflow temperatures (>450°C), providing better-than-expected visual results of flux residue! Solder fluxes have not traditionally been

Products

Solving Solder Starvation in SMT Electronics Assembly

Solder starvation is a serious electronics assembly issue – with a very simple solution. Solder starvation occurs when adequate volumes of solder are not available to effect a perfectly-shaped

Products

Humidity and Solder Paste Do Not Mix

Unbeknowst to me, the refrigerator where I store my solder paste and fluxes that I use for SIR (Surface Insulation Resistance) testing was being moved. One of my colleagues showed up at my desk with

Products

Lead Use on the Rise, Bismuth Supplies Secure: Solder Alloy Considerations

Based on a recent post I published regarding the use of bismuth (Bi)in solder alloys, John writes: "If Bismuth comes from the production of Pb, and if the use of Pb is being reduced, won’t

Archive

Solar Cell Testing

As a tech guy, I couldn’t be more excited about testing these 8 different c-Si solar cell / metallization designs! Why? Well, testing at customer sites is limited to only a few cell types

Products

Bismuth Solder Alloy Follow On

Folks, A few people asked some questions after my last post on bismuth solders.Here they are: 1. The low melting point of these solders is encouraging.What are realistic field use conditions? Bismuth

Support

The Limits of Aqueous Flip-Chip Cleaning (I)

This post was prompted by a Korean customer, who this month asked what thelimitations are for aqueous (water-based) cleaning for fluxes used in copper-pillar flip-chip applications. How low can the

Archive

Options for Attaching Power Amplifiers: Soldering & Thermal Management

Power amplifiers and transistors come in many shapes and sizes. The performance requirements vary as well. Attaching them can be a critical aspect of your design. Both Pb and Pb-free alloys can be

Archive

Heat-Spring® Thermal Interface Video Release

Sampling, receiving, and testing indium Heat-Spring® compressible thermal interface materials are easier than ever!Not only are standard samples (solder research bundle kits) available for

Products

The Secret Life of Engineers (Part 3 – Be a Rock Star)

In my last Secret Life of Engineers post I mentioned that you will need to travel to become a true expert in your field of

Products

Has the Time Come for Tin-Bismuth Solders?

Folks, When the industry was preparing to transition to lead-free solders almost ten years ago (can it have been that long), tin-bismuth solders were serious candidates.Their low melting point, of

Support

The Secret Life of Engineers (Part 2 – Travel)

I always imagined being an engineer would require me to sit in front of the same computer, in the same chair, in the same room, day after day after… (you get the point). Not only was this a

Support

Engineering Functions and the Secret Life of Engineers

A few weeks ago Brandon Judd and I had an opportunity to show 4 middle/high school students what it is like to be an engineer. In preparation, we decided the curriculum should be ‘what everyone

At Indium we research, develop, and manufacture advanced electronics assembly materials solutions to the challenges of today, tomorrow, and the future.