Trade Show Travels June 2022

June has been a busy month for the semiconductor team at Indium Corporation. Earlier this month the team traveled to ECTC in San Diego California, the premier international event bringing together

Products

Square vs. Circular Apertures and the Five Ball Rule Revisited

Folks, I recently posted that circular apertures deliver much less solder paste than square apertures. One of the obvious reasons is that a circle of diameter D has only 78.5% of the area of a square

Products

Solder Failure Analysis

A colleague once told me, “You can’t cheat physics.” Of course, this wasn’t a novel concept to either of us, but itwas in the context of our conversation that made it a

Archive

Thank You Indium Corporation!

Man have these 10 weeks flown by! Today marks the final day of my internship at Indium Corporation. I am beyond grateful for this opportunity that was offered to me. I will admit I was very nervous

Archive

Analyzing a Stress-Strain Curve

Tensile strength is an important physical measurement that represents the maximum amount of force a specific material can undergo before fracturing/ breakage. Tensile strain is another important

Archive

Industry Back to Academia

With my internship here at Indium Corporation coming to an end, it’s nice to reflect back on all that I’ve done in my short time here and thank all the great people I met along the way.

Archive

Start Something Great!

During my internship here at Indium Corporation, I have had the chance to meet and talk with so many wonderful people within the company. From executives and managers to lab techs and my fellow

Products

Indium Corporation and SAFI-Tech Announce Partnership in Very Low Temperature Solders

Folks, Soldering is one of the oldest technologies developed by humankind, perhaps as long as 6,000 years ago. Early uses were in the making of jewelry, cookware, utensils, and weapons. Metals such

Products

The Importance of an Oxygen Barrier In Solder Paste Flux

Folks, Solder paste is arguably one of the most highly engineered materials. What is usually called solder paste “flux” is a combination of activators that dissolve oxides off metal

Archive

Power Grids in a Changing World – The Future

While my two previous blog posts made our current situation seem very dim, there are power grid solutions available to light the path for the future. These solutions are already commercially

Archive

Indium Marathon Driver: A Travel Blog

When I first started at Indium Corporation, I was full of excitement and determination. In fact, I was so focused on the end goal of my project. I did not even think about what challenges I may come

Archive

We’re Half Way There

What an amazing experience so far! I am a little more than half way through my ten-week internship here at Indium Corporation, and I have learned so much. Coming from a heavy academia background at

Archive

Indium Corporation: One Big Team!

If I were asked to describe working in Human Resources (HR) at Indium Corporation in one word, I would choose “teamwork.” Well, I might also be inclined to say "fun",

Archive

‘In’ our history: Top secret process for propeller blades

In mid-October 1943, the Chicago Bears were on their way to a 19-1-1[1] record over the course of two seasons (a record all the more impressive considering 45 active members from the undefeated 1942

Products

Celebrating Women in Science at Indium Corporation!

Join us as we’re introducing our latest series, “Celebrating Women in

Archive

Dancing our Way to Dead Last

A word of advice – if you’re planning on competing in a local scavenger hunt, you might want to find some teammates who know the area. And have an action plan. And maybe don’t walk

Archive

Conquering Interview Anxiety: Don’t Let Fear Get in the Way of Your Dreams

I still remember my first interview; it was for a part-time job at Olympia Sports when I was 16, and I was absolutely terrified. I have always been somewhat of a strong writer because writing gives

Products

Excel Software Tool to Determine Mass Fractions in Binary Alloy

Folks, Recently, I posted a derivation of the equations to determine the mass fractionsof two metals in a binary alloy. I thought it may be helpful to develop an Excel software tool to perform these

Support

Cutting out the cutting tool in the PBF process

“When the year 2000 was upon us, books were written and people were philosophizing on what the greatest invention was of the last 1,000 years. And almost all people agreed that the greatest

Archive

Academia to Industry: Project Management

Saying I graduate in the spring of 2023 use to sound so far away, but now, it’s less than a year away. I was hoping to get some experience in the workplace before I graduated and Indium

At Indium we research, develop, and manufacture advanced electronics assembly materials solutions to the challenges of today, tomorrow, and the future.