Indium Corporation is a global leader in high-purity tin and tin-based alloys and compounds. With unmatched expertise in sourcing, processing, and manufacturing, we deliver reliable and efficient solutions to meet the diverse needs of each customer.

Powered by Indium Corporation

  • High Purity From 3N to 6N
  • Decades of Experience
Various high purity tin metal bars and a cylindrical piece displayed on a white surface.

Wide Portfolio

Our tin products are designed for industrial use with purity levels from 3N5 to 6N. We provide ingots and shots in different sizes and shapes for versatile applications. And our high-purity offerings meet strict requirements for tasks like tin plating, e-beam evaporation, and EUV plasma generation.

Quality Assurance

Backed by a robust quality management system, our tin products adhere to stringent quality standards, guaranteeing compliance with precise material property criteria. Expect superior quality with ultra-low bulk oxygen content and minimal surface oxide thickness.

Typical Impurities

Due to its ductility, malleability, and electronic properties, tin is widely utilized in the electronics industry, frequently in alloy form. Pure tin provides the optimal plasma spectrum for EUV generation in the semiconductor sector.

3N5 to 6N

99.9999%

Available Physical Forms

  • Ingot
  • Shot
  • Powder
  • Customer fabrications (sphere, wire, tubing, and more)

Grades Available

  • 3N5
  • 4N
  • 4N8
  • 5N
  • 6N
PropertyValue
Atomic Weight 118.71
Melting Point 505.08 K (231.93°C or 449.47°F)
Boiling Point 2,875 K (2,602°C or 4,715°F)
Density 7.29 g/cm³ (β tin), 5.77 g/cm³ (α tin), 6.97 g/cm³ (liquid at MP)
Phase at Room Temperature Solid
Vapor Pressure 986 x 10⁻⁶ Pa at 1,000°C
Surface Tension 544 mN/m at MP
Viscosity at Melting Point 1.85 m·Pa (cP)
Specific Heat @ 20°C 222 J/(kg·K)
Latent Heat of Fusion 14.2 cal/g
Thermal Conductivity @ 20°C 65 W/(m·K)
Coefficient of Linear Expansion 19.9 x 10⁻⁶ at 0°C
Shrinkage on Solidification 2.80%
Volume Conductivity 15 IACS
Brinell Hardness @ 20°C 3.9 (10kg, 5mm, 180s)
Tensile Strength @ 15°C 2,100 psi
Latent Heat of Vaporization 520 +/- 20 cal/g

Product Data Sheets

Commercial Tin Metal PDS 98803 (A4) R0.pdf
Commercial Tin Metal PDS 98803 R0.pdf

Related Applications

Metal frames being treated with an electroplating kit in a factory setting with several tanks.

Electroplating

Try indium electroplating to enhance appearance and…

Microchips on a printed circuit board

PCB Assembly

Proven and cutting-edge materials for PCB assembly…

Related Markets

Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!

This image has an empty alt attribute; its file name is scientist-with-microscope.png

Looking for Safety Data Sheets?

Access everything you need — from technical specifications to application guidance — in one convenient location.