I just wanted to take a second and mention my affection for water soluble fluxes they make my life easier! If you've ever used a spin coat machine (spinner) to apply a polymer or flux on a wafer, you know it makes quite a mess. The whole theory behind spin coating is to fling excess liquid off the wafer (and consequently onto the inside of the machine). Being able to simply use a water bottle and a wet paper towel to clean the machine is a lot more desirable to me than using a solvent like alcohol. Who wants to smell IPA?
Related Articles
From Scrap to Savings: Indium Corporation’s Commitment to a Sustainable World
In today's fast-paced world, where sustainability and environmental responsibility are paramount, Indium Corporation is leading the charge with an innovative approach to resource management. Our
Unlock Savings with Indium Corporation’s Reclaim and Recycle Program
Navigating today’s competitive business landscape demands innovative strategies for cost management and operational efficiency. Indium Corporation's Reclaim and Recycle Program addresses
Demystifying Recycling and Reclaiming: A Guide to Sustainable Practices
Unlock new efficiencies in your manufacturing process with Indium Corporation's Reclaim and Recycle Program—a visionary approach that turns post-manufacturing scrap into valuable resources.