Bỏ qua nội dung

Indium Corporation Features Ultra-Low Residue No-Clean Flip-Chip Flux at IMAPS

Indium Corporation will feature NC-26-A Ultra-Low Residue No-Clean Flip-Chip Flux at the 47th International Symposium on Microelectronics, organized by the International Microelectronics Assembly and Packaging Society (IMAPS), Oct. 14-16 in San Diego, Calif.

NC-26-A is a halogen-free, no-clean flip-chip dipping flux designed to leave a clear, undetectable residue that allows the manufacturer to eliminate the cleaning process.

NC-26-A controls wetting activity to better avoid two main soldering issues that plague manufacturing engineers: solder bridging and cold joints. NC-26-A also retains its bump height after reflow, reduces the UBM/bump crack caused by vibration in the cleaning process, and boasts a higher compatibility with capillary and molded underfills (CUF and MUF).

NC-26-A is designed for flip-chip dipping applications and has tackiness suitable for holding die in mass-reflow assembly processes. For more information on NC-26-A, visit indiumstg.wpenginepowered.com/no-clean-flip-chip-fluxes or visit Indium Corporation at booth 217.

Indium Corporation là nhà sản xuất và cung cấp vật liệu hàng đầu cho các thị trường điện tử, bán dẫn, năng lượng mặt trời, màng mỏng và quản lý nhiệt toàn cầu. Các sản phẩm bao gồm chất hàn và chất trợ dung; hàn đồng; vật liệu giao diện nhiệt; mục tiêu phun; kim loại indium, gali, germani và thiếc và các hợp chất vô cơ; và NanoFoil ® . Được thành lập vào năm 1934, Indium có hỗ trợ kỹ thuật toàn cầu và các nhà máy đặt tại Trung Quốc, Malaysia, Singapore, Hàn Quốc, Vương quốc Anh và Hoa Kỳ.

Để biết thêm thông tin về Indium Corporation, vui lòng truy cập trang web indiumstg.wpenginepowered.com hoặc gửi email đến địa chỉ [email protected].