Indium Corporation will feature NC-26-A Ultra-Low Residue No-Clean Flip-Chip Flux at the 47th International Symposium on Microelectronics, organized by the International Microelectronics Assembly and Packaging Society (IMAPS), Oct. 14-16 in San Diego, Calif.
NC-26-A is a halogen-free, no-clean flip-chip dipping flux designed to leave a clear, undetectable residue that allows the manufacturer to eliminate the cleaning process.
NC-26-A controls wetting activity to better avoid two main soldering issues that plague manufacturing engineers: solder bridging and cold joints. NC-26-A also retains its bump height after reflow, reduces the UBM/bump crack caused by vibration in the cleaning process, and boasts a higher compatibility with capillary and molded underfills (CUF and MUF).
NC-26-A is designed for flip-chip dipping applications and has tackiness suitable for holding die in mass-reflow assembly processes. For more information on NC-26-A, visit indiumstg.wpenginepowered.com/no-clean-flip-chip-fluxes or visit Indium Corporation at booth 217.
Indium Corporation is a premier materials manufacturer and supplier to the global electronics, semiconductor, solar, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, Indium has global technical support and factories located in China, Malaysia, Singapore, South Korea, the United Kingdom, and the USA.
For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email [email protected].