Indium Hydroxide
Indium hydroxide is a white, odorless powder that is highly soluble in acids but only slightly soluble in water. This compound, which is offered in both fine and crystalline forms, plays a vital role in crafting indium-based materials, primarily serving as a precursor for synthesizing various indium compounds such as indium oxide. We carefully produce indium hydroxide under stringent quality control measures, ensuring a consistent performance across all applications.
Powered by Indium Corporation
- High Purity Levels of 4N (99.99%) to 5N (99.999%)
- Rigorous Quality Control
- Available in Two Forms
Features
Indium Hydroxide Products
Indium hydroxide is available in two forms to meet diverse needs: Type A offers high purity and stability for precision applications, while Type B’s fine powder enhances reactivity, making it ideal for catalysts and chemical synthesis.
| Property | Indium Hydroxide Type A (Crystalline Powder) | Indium Hydroxide Type B (Fine Powder) |
|---|---|---|
| Description | High purity, structurally stable crystalline powder, suitable for high-precision applications like electronics and optical devices | Fine powder with heightened reactivity, ideal for catalysts and chemical synthesis |
| Appearance | White powder | White powder |
| Purity Grades | 4N (99.99%), 5N (99.999%) | 4N (99.99%), 5N (99.999%) |
| Nominal Indium Percentage | 68.8 ± 0.9% | 65.6 ± 1.7% |
| Particle Size Distribution (d90) | 15.0–46.0μm | 1.1–7.2μm |
| Particle Size Distribution (d50) | 8.9–28.0μm | 1.4–2.5μm |
| Particle Size Distribution (d10) | 1.6–14.0μm | 0.8–1.1μm |
| BET Surface Area | 5.7m²/g (typical) | 50–65m²/g (typical) |
Related Applications
Indium hydroxide is suitable for a variety of applications.
Related Markets
Indium Corporation’s indium hydroxide is available for use in the following markets:
Expert Support for Reliable Results
Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!
Looking for Safety Data Sheets?
Access everything you need — from technical specifications to application guidance — in one convenient location.
Your Success
is Our Goal
Optimize your processes with the latest materials, technology, and expert application support. It all starts by connecting with our team.