Thermal Interface Materials
Liquid Metal and Liquid Metal Pastes
Indium Corporation’s liquid metals are pure metals, or metal alloys, that remain liquid at room temperature, with melting points between 7.6°C and 17°C. These alloys are primarily gallium-based, often combined with elements like indium, tin, or zinc. All our liquid metals are RoHS-compliant, non-toxic, and can be transported globally in full compliance with shipping regulations.
Liquid Metal Properties
- Liquid at Room Temperature
- High Thermal Conductivity
- Non-Toxic, Gallium-Based Materials

Product Overview
Wets to Many Surfaces
Liquid metals wet to most metallic and non-metallic surfaces through two mechanisms—oxide pinning, a physical bond of an oxide to a relatively smooth surface, and reactive wetting, a metallurgical bond.
Liquid at Room Temperature
Gallium-based metals have excellent thermal conductivity, making them an ideal thermal interface material. As high-density, low viscosity materials, these substances form a thin, self-limiting oxide layer on their surface when exposed to air.
Higher Temperature, Higher Thermal Conductivity
Another interesting property of gallium-based liquid metals is that their thermal conductivity increases with temperature, meaning that the thermal performance of liquid metal TIMs improves as well.
Electrically Conductive
Liquid metals are electrically conductive and must be contained to prevent leakage or shorts in electronics. Indium Corporation’s patented multi-barrier system ensures compatibility, corrosion resistance, flexibility, and durability with gallium-based materials.
Indium Corporation’s Patented Multi-Barrier System for Liquid and Hybrid Liquid Metals

Features
Liquid Metal and Liquid Metal Paste Products
Product Data Sheets
Liquid Metal Gallium and Gallium Alloys PDS 97826.pdf
Liquid Metal TIMs PDS 99939 R2.pdf
LMP Liquid Metal Paste PDS 100021 R3.pdf
m2TIM™ and Liquid Metal Thermal Interface Materials PDS 99600 R4.pdf
Related Applications
Liquid metal and liquid metal paste products are suitable for a variety of applications.
Related Markets
Indium Corporation’s liquid metal and liquid metal paste products are available for use in a wide range of markets.
Expert Support for Reliable Results
Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!

Looking for Safety Data Sheets?
Access everything you need — from technical specifications to application guidance — in one convenient location.

Your Success
is Our Goal
Optimize your processes with the latest materials, technology, and expert application support. It all starts by connecting with our team.