Products Alloys Solder Alloys

Solder Alloys

Since our founding in 1934, Indium Corporation has been a global leader in specialty solders and alloy development. Our research and development team, which includes many Ph.D. metallurgists, collaborates on our core metals to develop alloys that tackle current and emerging soldering and sealing challenges.

Powered by Indium Corporation

  • Patented Alloy Technologies
  • World-Class Development Team and Labs
  • 90+ Years of Experience
Various solder alloys

Application Expertise

Our global applications engineering teams are available for consultations to fully understand your unique needs.

Various Forms

Most solder alloys can be supplied in the form of pastes, preforms, wires, bars, spheres, and more.

Mixed Alloy Technology

Our patented mixed alloy technology, Durafuse®, tackles the latest soldering challenges. Since its introduction, multiple products featuring this technology have evolved and been adopted by major OEMs, EMS providers, and OSATs.

Liquid Metal for Thermal Interface (<30ºC)

  • Indalloy® 51E (GaInSn)
  • Indalloy® 60 (GaIn)
  • Indalloy® 77 (GaIn)
  • Indalloy® 300E (GaIn)

Low-Temperature Solder and Sealing (30–210ºC)

  • Indalloy® 1E (InSn)
  • Indalloy® 4 (In)
  • Indalloy® 38 (BiPbSn)
  • Indalloy® 117 (BiPbInSnCd)
  • Indalloy® 227 (SnInAg)
  • Indalloy® 254 (SnInAg)
  • Indalloy® 281 (BiSn)
  • Indalloy® 282 (BiSnAg)

Traditional Soldering (150–260ºC)

  • Indalloy® 100 (SnPbAg)
  • Indalloy® 106 (Sn63)
  • Indalloy® 121 (SnAg)
  • Indalloy® 241 (SAC387)
  • Indalloy® 256 (SAC305)
  • Indalloy® 276 (SnAg+)
  • Indalloy® 291 (SnCu+)

High-Temperature Soldering (230–360ºC)

  • Indalloy® 133 (SnSb)
  • Indalloy® 228 (Sn10)
  • Indalloy® 266 (HMP)
  • Indalloy® 292

Au and Braze Alloys (>280ºC)

  • Indalloy® 182 (AuSn)
  • Indalloy® 183 (AuGe)
  • Indalloy® 193 (AgCu)
  • Indalloy® 200 (Au)

Six Solder Alloy Families

Gallium

Indalloy® #CompositionLiquidus/Solidus Temperature (°C)
51E66.5Ga/20.5In/13Sn11 Eutectic
300E78.6Ga/21.4In15.7 Eutectic

Bismuth

Indalloy® #CompositionLiquidus/Solidus Temperature (°C)Solidus Temperature (°C)
28158Bi/42Sn138 Eutectic
28257Bi/42Sn/1Ag140139

Indium

Indalloy® #CompositionLiquidus/Solidus Temperature (°C)Solidus Temperature (°C)
1E52In/48Sn118 Eutectic
150In/50Sn126118
29097In/3Ag143 Eutectic
280In/15Pb/5Ag154149
4100In157 Melting point
20470In/30Pb175165
20560In/40Pb181173
22777.2Sn/20In/2.8Ag187
750In/50Pb210184
390In/10Ag237143
16492.5Pb/5In/2.5Ag310300

Tin

Indalloy® #CompositionLiquidus/Solidus Temperature (°C)Solidus Temperature (°C)
10663Sn/37Pb (Sn63)183 Eutectic
12196.5Sn/3.5Ag221 Eutectic
13395Sn/5Sb240237
25696.5Sn/3Ag/0.5Cu (SAC305)220217

Lead

Indalloy® #CompositionLiquidus/Solidus Temperature (°C)Solidus Temperature (°C)
15192.5Pb/5Sn/2.5Ag306298
16492.5Pb/5In/2.5Ag310300

Gold

Indalloy® #CompositionLiquidus/Solidus Temperature (°C)Solidus Temperature (°C)
18280Au/20Sn280 Eutectic
18388Au/12Ge356 Eutectic
18496.8Au/3.2Si363 Eutectic
200100Au1,064 Melting Point

Solder Alloy Guide

Looking for a specific alloy? Visit our Solder Alloy Selector Guide to figure out which Indium Corporation alloy is right for your application, or download our Solder Alloy Directory to browse the available Indalloys.

Solder Alloy Directory 97720 (A4) R9.pdf

Related Applications

Microchips on a printed circuit board

PCB Assembly

Proven and cutting-edge materials for PCB assembly

Futuristic white car with advanced power electronics zips through a neon-lit city at night, showcasing cutting-edge speed and technology.

Power Electronics Packaging & Assembly

Extensive range of proven high-reliability solder and more

High Temperature Soldering

High-Temperature Soldering

Offering high-temperature soldering materials for critical applications in harsh

Related Markets

Solder alloys are widely used in industries that involve electronics assembly or packaging.

Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!

This image has an empty alt attribute; its file name is scientist-with-microscope.png

Looking for Safety Data Sheets?

Access everything you need — from technical specifications to application guidance — in one convenient location.