SOLDER Preforms
InFORMS® Reinforced Preforms
Reinforced solder preforms are designed to enhance solder joint reliability by adding strength, delivering consistent bondline thickness, and reducing stress concentrations in the interface.
Powered by Indium Corporation
- Uniform Bondline Thickness
- Improved Fatigue Resistance
- Even Stress Distribution
Product Overview
Reinforced Matrix for Precision Bondline Control
InFORMS® provide superior bondline consistency with an integrated matrix standoff, offering better control compared to single-point solutions susceptible to movement.
Mechanical Strengthening
InFORMS® remain within the solder after reflow, reinforcing the interface to resist solder creep, enhance fatigue resistance, and improve solder joint lifecycle reliability.
Customizable for Each Application
InFORMS® solder preforms are available in standard and custom shapes with precise tolerances, offering flexible matrix configurations for optimal design compatibility.
Compatible with a Wide Range of Solder Alloys
Leveraging Indium Corporation’s extensive alloy library, InFORMS® can be customized with or without flux-coating for increased reliability and repeatability in various applications.
Quick Facts
InFORMS® are specifically developed to realize superior solder joint reliability in a variety of applications.
Reinforced Preforms Products
InFORMS® reinforced solder preforms are available in various configurations, which can be selected based on the target design requirements for part dimensions and bondline thickness.
Solder Preform Requirements
| Description | Approximate Standoff (Microns) | Part Dimensions (x and y) per side (Millimeters) | Part Dimensions (z) (Microns) |
|---|---|---|---|
| ESM02 | 55 | 1.9-3.5 | >110 |
| ESM03 | 80 | 1.9-3.5 | >140 |
| SM04 | 110 | 3.5-11 | >165 |
| LM04 | 110 | >11 | >165 |
| LM06 | 165 | >11 | >215 |
| LM08 | 215 | >11 | >280 |
| ESM10 | 265 | 1.9-3.5 | >330 |
Product Data Sheets
InFORMS® PDS 97548 R14.pdf
Indalloy®301LT for Preforms and InFORMS® PDS 100089 R3.pdf
AuLTRA® ThInFORMS® for Die-Attach Applications PDS 99803 R1.pdf
InFORMS® Reinforced Indium and Solder Alloy Fabs PDS 99297 (SC A4) R0.pdf
Related Applications
Related Markets
Expert Support for Reliable Results
Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!
Looking for Safety Data Sheets?
Access everything you need — from technical specifications to application guidance — in one convenient location.
Your Success
is Our Goal
Optimize your processes with the latest materials, technology, and expert application support. It all starts by connecting with our team.