This video is for electronics assembly professionals who are looking to improve their wave soldering processes. It includes tools and resources that will help overcome common challenges.
Phil Zarrow: Wave soldering: It's been around for over 70 years, just won't go away, and for a lot of people it still causes problems. Dr. Lasky, I understand you've developed a tool that engineers, technicians, and managers can help use to alleviate some of the anxiety caused by wave soldering.
Dr. Ronald C. Lasky: I'm sure you're not surprised, Phil, when you go out and do audits, that, very seldom does the thermal profile on the wave soldering machine match the flux specifications. So, I developed a software tool in which you enter the values from the flux specification, and the temperature and time values from your thermal profile, and it analyzes these to see if you've matched the flux specification.
Phil Zarrow: What does the output look like?
Dr. Ronald C. Lasky: There is a red line and a blue line that are what the flux specification is asking for. Then your thermal input is a green line. As long as the green line is within the red and blue lines, you've matched the flux specification, and you're hopefully on your way to terrific wave soldiering.
Phil Zarrow: It sounds very straightforward and very useful. Where can we find this tool?
Dr. Ronald C. Lasky:You find the tool at www.indium.com.
Phil Zarrow: Excellent. Dr. Lasky, thank you very much.
Keywords: indium, Indium Corporation,Dr. Ron Lasky, [email protected], Phil Zarrow, [email protected], wave soldering, waveCoach, thermal profile, flux specifications
Our blogging team includes engineers, researchers, product specialists, and industry leaders. We share expertise in solder materials, electronics assembly, thermal management, and advanced manufacturing. Our blog offers insights, technical knowledge, and solutions to inspire professionals, showcasing product innovations, trends, and best practices to help readers excel in a competitive industry.
Professor Patty Coleman was in her office at Ivy University contemplating a truism. Both she and her husband Rob worked at Ivy U, but they couldn’t afford to send their twin sons
Ivy University Professor Patty Coleman was at Simon Pearce Restaurant, having a solo lunch and relaxing as she watched the beautiful waterfall at the restaurant. As she enjoyed their signature
When it comes to electronics reliability, surface insulation resistance (SIR) testing is one of the most important, yet often overlooked, safeguards. Failures in SIR can lead to mission losses,