Indium Corporation Features SACm at SMTAi: New, High-Reliability Solder Alloy Reduces Drop-Shock Performance by 800%

September 5, 2013

Indium Corporation will feature its new technology platform using the SACm™ Solder Alloy at Surface Mount Technology Association International (SMTAi) October 15-17 in Fort Worth, Texas.

SACm™ is a high-reliability solder alloy that offers drop-shock test performance far superior to other SAC alloys, without compromising on thermal cycling. Its low silver content makes it a cost-effective solution for portable electronics.

The platform consists of Indium8.9 Series solder pastes using Indium Corporation’s patent-pending SACm™ solder alloy technology for board-side interconnect, and SACm™ solder balls (spheres) for package-level interconnect.

Dr. Ning-Cheng Lee, Vice President of Technology, said, SACm™ offers a fine grain size with a thin, stable IMC layer, even after exposure to accelerated life conditions.

“We see a fine grain size with a thin, stable IMC layer, even after exposure to accelerated life conditions,” Dr. Lee said. “These micro-structural improvements translate into an 8X (800%) improvement in drop-shock performance and 50% extension in thermal cycling.”

SACm™ is doped with manganese and contains less silver than other Pb-free alloys. Manganese provides increased strength. The reduced silver content provides a more stable cost structure, especially beneficial for cost-sensitive applications.

Indium Corporation will be exhibiting at booth 318.

For more information about Indium Corporation’s SACm™ solder paste, visit SACm or email [email protected].