Indium Corporation has released IndiOx™ (In2O3) for use in the manufacture of ITO sputtering targets for thin-film coating. IndiOx™ (In2O3) is a stable ceramic-like material that is insoluble in water and volatizes at 850°C.
When doped with tin oxide, IndiOx™ forms ITO, the material of choice to form transparent conductive oxide (TCO) layers in flat-panel displays and touch sensors for mobile devices. The ITO layer is deposited onto glass from a sputtering target that is manufactured from the ITO powder by sintering.
Other uses for IndiOx™ include glass coloring, gassing suppression in alkaline batteries, and as an anti-arcing additive in high current electrical switches and contactors.
IndiOx™ is available in three powder types:
- Type A – Crystalline: particle size distribution D10–D90 ranges from 0.8–38μm.
- Type B – Fine: particle size distribution D10–D90 ranges from 0.5–6μm.
- Type T – Target Grade: particle size distribution D10–D90 ranges from 0.1–7.5μm. The primary particle size is about 100nm.
For more information about Indium Corporation’s suite of compound materials, visit indiumstg.wpenginepowered.com/indiox.
Indium Corporation è uno dei principali produttori e fornitori di materiali per i mercati globali dell'elettronica, dei semiconduttori, dei film sottili e della gestione termica. I prodotti includono saldature e flussanti, brasature, materiali per interfacce termiche, target per sputtering, metalli e composti inorganici di indio, gallio, germanio e stagno e NanoFoil®. Fondata nel 1934, l'azienda dispone di un'assistenza tecnica globale e di stabilimenti situati in Cina, India, Malesia, Singapore, Corea del Sud, Regno Unito e Stati Uniti.