Products Alloys Solder Alloys

Solder Alloys

Since our founding in 1934, Indium Corporation has been a global leader in specialty solders and alloy development. Our research and development team, which includes many Ph.D. metallurgists, collaborates on our core metals to develop alloys that tackle current and emerging soldering and sealing challenges.

Powered by Indium Corporation

  • Patented Alloy Technologies
  • World-Class Development Team and Labs
  • 90+ Years of Experience
Various solder alloys

Application Expertise

Our global applications engineering teams are available for consultations to fully understand your unique needs.

Various Forms

Most solder alloys can be supplied in the form of pastes, preforms, wires, bars, spheres, and more.

Mixed Alloy Technology

Our patented mixed alloy technology, Durafuse®, tackles the latest soldering challenges. Since its introduction, multiple products featuring this technology have evolved and been adopted by major OEMs, EMS providers, and OSATs.

Liquid Metal for Thermal Interface (<30ºC)

  • Indalloy® 51E (GaInSn)
  • Indalloy® 60 (GaIn)
  • Indalloy® 77 (GaIn)
  • Indalloy® 300E (GaIn)

Low-Temperature Solder and Sealing (30–210ºC)

  • Indalloy® 1E (InSn)
  • Indalloy® 4 (In)
  • Indalloy® 38 (BiPbSn)
  • Indalloy® 117 (BiPbInSnCd)
  • Indalloy® 227 (SnInAg)
  • Indalloy® 254 (SnInAg)
  • Indalloy® 281 (BiSn)
  • Indalloy® 282 (BiSnAg)

Traditional Soldering (150–260ºC)

  • Indalloy® 100 (SnPbAg)
  • Indalloy® 106 (Sn63)
  • Indalloy® 121 (SnAg)
  • Indalloy® 241 (SAC387)
  • Indalloy® 256 (SAC305)
  • Indalloy® 276 (SnAg+)
  • Indalloy® 291 (SnCu+)

High-Temperature Soldering (230–360ºC)

  • Indalloy® 133 (SnSb)
  • Indalloy® 228 (Sn10)
  • Indalloy® 266 (HMP)
  • Indalloy® 292

Au and Braze Alloys (>280ºC)

  • Indalloy® 182 (AuSn)
  • Indalloy® 183 (AuGe)
  • Indalloy® 193 (AgCu)
  • Indalloy® 200 (Au)

Six Solder Alloy Families

Gallium

Indalloy® #CompositionLiquidus/Solidus Temperature (°C)
51EGa66.5/In20.5/Sn1311 Eutectic
300EGa78.6/In21.415.7 Eutectic

Bismuth

Indalloy® #CompositionLiquidus/Solidus Temperature (°C)Solidus Temperature (°C)
281Bi58/Sn42138 Eutectic
282Bi57/Sn42/Ag1140139

Indium

Indalloy® #CompositionLiquidus/Solidus Temperature (°C)Solidus Temperature (°C)
1EIn52/Sn48118 Eutectic
1In50/Sn50126118
290In97/Ag3143 Eutectic
2In80/Pb15/Ag5154149
4In100157 Melting Point
204In70/Pb30175165
205In60/Pb40181173
227Sn77.2/In20/Ag2.8187
7In50/Pb50210184
3In90/Ag10237143
164Pb92.5/In/Ag2.5310300

Tin

Indalloy® #CompositionLiquidus/Solidus Temperature (°C)Solidus Temperature (°C)
106Sn63/Pb37 (Sn63)183 Eutectic
121Sn96.5/Ag3.5221 Eutectic
133Sn95/Sb5240237
256Sn96.5/Ag3/Cu0.5 (SAC305)220217

Lead

Indalloy® #CompositionLiquidus/Solidus Temperature (°C)Solidus Temperature (°C)
151Pb92.5/Sn5/Ag2.5306298
164Pb92.5/In5/Ag2.5310300

Gold

Indalloy® #CompositionLiquidus/Solidus Temperature (°C)Solidus Temperature (°C)
182Au80/Sn20280 Eutectic
183Au88/Ge12356 Eutectic
184Au96.8/Si3.2363 Eutectic
200Au1001,064 Melting Point

Solder Alloy Guide

Looking for a specific alloy? Visit our Solder Alloy Selector Guide to figure out which Indium Corporation alloy is right for your application, or download our Solder Alloy Directory to browse the available Indalloys.

Related Applications

Microchips on a printed circuit board

PCB Assembly

Proven and cutting-edge materials for PCB assembly…

Futuristic white car with advanced power electronics zips through a neon-lit city at night, showcasing cutting-edge speed and technology.

Power Electronics Packaging & Assembly

Extensive range of proven high-reliability solder and…

High Temperature Soldering

High-Temperature Soldering

Offering high-temperature soldering materials for critical applications…

Related Markets

Solder alloys are widely used in industries that involve electronics assembly or packaging.

Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!

This image has an empty alt attribute; its file name is scientist-with-microscope.png

Looking for Safety Data Sheets?

Access everything you need — from technical specifications to application guidance — in one convenient location.