When it comes to shots at Indium Corporation, it is not about bullets, vaccines, or vodka; it’s about small spherical or tear-drop shaped forms of metals and alloys. While ingots and cakes are more popular forms when we think about metals and alloys, shots have their exclusive benefits.
Shots provide a larger area-to-volume ratio for the metals and alloys that favor the interaction with external factors. Afterall, dissolving a certain volume of metal in a solution is much easier and faster with small pieces than with a single bulk quantity. For instance, considering a 500g indium ingot with dimensions of 7” × 1.25” × 0.5” versus several indium shots of 0.125” diameter with the same total weight, the ratio of surface area exposed to the solution is nearly 8 times higher for shots. Therefore, if surface area is the limiting factor in dissolving indium in a chemical solution, shots would ideally dissolve 8 times faster.
I tecnici che utilizzano vasche di fusione più piccole troveranno utile l'uso di shot quando i lingotti sono troppo grandi per essere inseriti. I pallini offrono una migliore risoluzione della quantità di alimento. È possibile pesare facilmente i pallini per ottenere quantità più precise, cosa difficile da ottenere con metalli e leghe in forme più grandi. Inoltre, aiuta a ridurre gli scarti ottenuti dopo la limatura dei lingotti. Inoltre, lo stoccaggio, la manipolazione e l'alimentazione sono molto più convenienti con metalli e leghe di forma sferica o a goccia.
I pallini sono prodotti in genere forzando la forma fusa del metallo attraverso piccole aperture circolari. Il metallo fuso passa quindi in una soluzione di raffreddamento e si solidifica in pallini. I pallini vengono essiccati, ricotti o ulteriormente lavorati per ottenere stabilità e indurimento. Le dimensioni delle aperture circolari e la lunghezza del passaggio attraverso la soluzione determinano le dimensioni e la forma dei pallini.
Shots in general have a lower shelf-life compared to larger-sized forms because of the larger exposed area, which increases the interaction with external elements like oxygen, humidity, etc.
Indium Corporation produces spherical and tear-drop shaped shots for different metals and alloys. This list includes, but is not limited to, indium, gallium, germanium, tin, Indalloy®117, Indalloy®136, and Indalloy®158. The purity that we provide ranges from 3N to 6N5. Readily available shots are approximately 0.125” in diameter and can be adjusted based on customer requirements and quantity. We can also manage the uniformity in size as required.