Fusible alloys, known for their lower melting points compared to solder alloys, are easily liquefied with moderate heat, making them ideal for temporary solid state during processing or as temperature sensors, such as in fire detection sprinkler systems. Originally developed in the 19th century and known by names such as Field’s metal, Wood’s metal, and Rose’s metal, these alloys have evolved with modern materials technology to include precise compositions like Indalloy®117, Indalloy®158, and Indalloy®19, delivering consistent melting behavior across an extended temperature range.

Alimentato da Indium Corporation

  • Broad Alloy Portfolio and Formulation Depth
  • Materials Science and Process Support
  • Leading Global Supplier of Fusible Alloys
Blocco delle lenti mediante leghe fusibili
Lens Blocking using Fusible Alloys or Low Melting Point Alloys

Panoramica del prodotto

Fusible alloys, characterized by their low melting points as low as 47°C (117°F), offer remarkable versatility by transitioning seamlessly between solid and molten states. This unique property makes them indispensable for precise and temporary applications. These alloys serve as excellent as precision support materials, securely holding and protecting workpieces during crucial finishing processes, such as polishing and grinding. Additionally, the eutectic melting points of fusible alloys facilitate passive activation systems, ensuring the reliable and safe operation of devices like fire sprinklers without the need for electronic circuitry, thereby enhancing safety and simplicity.

La più ampia gamma di composizioni di leghe disponibili

Field’s metal, Wood’s metal, and many other alloy compositions are available. Available melting points start at 47°C/117°F and go up into the solder alloy range at above 200°C.

Lens Blocking for Grinding and Polishing with Indalloy®117 & Indalloy®19

Indalloy®117 and Indalloy®19 are the most popular alloys for lens blocking in the optical lens grinding industry, with melt points at 47°C/117°F and 60°C/140°F, respectively.

Attivazione precisa dei sistemi antincendio a sprinkler

Melting activation is solely controlled by environmental temperature and thus enables the design of completely passive devices for fire detection. Indalloy®158 is a popular alloy choice for fire sprinkler systems.

Custom Alloy Development

Melting behavior is determined by precise control of the alloy composition. We offer a wide range of alloy options and melting points. We also work with customers to develop custom alloys with target melting points and other properties tailored to their application needs.

Dark green icon with stylized shapes and a dot on a white circular background.

Indalloy®117

Dark green icon with stylized shapes and a dot on a white circular background.

Indalloy®19 (Field’s Metal)

Dark green icon with stylized shapes and a dot on a white circular background.

Indalloy®158 (Wood’s Metal)

Dark green icon with stylized shapes and a dot on a white circular background.

Opzioni di lega senza piombo e cadmio

Indalloy #11713619158281
Composizione della lega44,7 Bi
22,6 Pb
19,1 In
8,3 Sn
5,3 Cd
49 Bi
21 In
18 Pb
12 Sn
51 In
32,5 Bi
16,5 Sn
50 Bi
26,7 Pb
13,3 Sn
10 Cd
58 Bi
42 Sn
Liquido in °C (°F)47 (117)58 (136)
60 (140)

60 (140)

138 (281)
E = EutetticoEEEEE

Applicazioni correlate

Le leghe fusibili/le leghe a basso punto di fusione sono adatte a un'ampia gamma di applicazioni.

Microchip su un circuito stampato

Assemblaggio di PCB

Materiali collaudati e all’avanguardia per l’assemblaggio di circuiti stampati…

Saldatura ad alta temperatura

Saldatura ad alta temperatura

Offering high-temperature soldering materials for critical applications…

Cilindro nero testurizzato con guarnizioni criogeniche, dotato di tre etichette rettangolari bianche sulla parte superiore.

Sigillatura: criogenica ed ermetica

Low temperature liquid & fusible alloys for…

Mercati correlati

Le leghe fusibili/le leghe a basso punto di fusione di Indium Corporation sono adatte a molti mercati.

Avete domande tecniche o richieste di vendita? Il nostro team dedicato è qui per aiutarvi. "Da un ingegnere all'altro®" non è solo il nostro motto: è il nostro impegno a fornire un servizio eccezionale. Siamo pronti quando lo siete voi. Mettiamoci in contatto!

Questa immagine ha un attributo alt vuoto; il suo nome file è scientist-with-microscope.png

Cercate le schede di sicurezza?

Accedete a tutto ciò che vi serve, dalle specifiche tecniche alle indicazioni per le applicazioni, in un'unica comoda posizione.