Products Compounds Indium Hydroxide

Indium Hydroxide

Indium hydroxide is a white, odorless powder that is highly soluble in acids but only slightly soluble in water. This compound, which is offered in both fine and crystalline forms, plays a vital role in crafting indium-based materials, primarily serving as a precursor for synthesizing various indium compounds such as indium oxide. We carefully produce indium hydroxide under stringent quality control measures, ensuring a consistent performance across all applications.

Powered by Indium Corporation

  • High Purity Levels of 4N (99.99%) to 5N (99.999%)
  • Rigorous Quality Control
  • Available in Two Forms
A pile of indium hydroxide sits as a white powder on a clear glass petri dish against a stark black background.
Dark green icon with stylized shapes and a dot on a white circular background.

In(OH)₃

Dark green icon with stylized shapes and a dot on a white circular background.

20661-21-6

Dark green icon with stylized shapes and a dot on a white circular background.

165.84g/mol

Dark green icon with stylized shapes and a dot on a white circular background.

69.24%

PropertyIndium Hydroxide Type A (Crystalline Powder)Indium Hydroxide Type B (Fine Powder)
DescriptionHigh purity, structurally stable crystalline powder, suitable for high-precision applications like electronics and optical devicesFine powder with heightened reactivity, ideal for catalysts and chemical synthesis
AppearanceWhite powderWhite powder
Purity Grades4N (99.99%), 5N (99.999%)4N (99.99%), 5N (99.999%)
Nominal Indium Percentage68.8 ± 0.9%65.6 ± 1.7%
Particle Size Distribution (d90)15.0–46.0μm1.1–7.2μm
Particle Size Distribution (d50)8.9–28.0μm1.4–2.5μm
Particle Size Distribution (d10)1.6–14.0μm0.8–1.1μm
BET Surface Area5.7m²/g (typical)50–65m²/g (typical)

Related Applications

Indium hydroxide is suitable for a variety of applications.

Factory where catalysis is used

Catalysis

Indium and gallium compounds for catalysis, chemical…

Molecular bonds showing chemical synthesis

Chemical Synthesis

Indium and gallium compounds for chemical synthesis…

Related Markets

Indium Corporation’s indium hydroxide is available for use in the following markets:

Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!

This image has an empty alt attribute; its file name is scientist-with-microscope.png

Looking for Safety Data Sheets?

Access everything you need — from technical specifications to application guidance — in one convenient location.