Indium Wire

Indium metal is ideal for soldering and sealing with its low melting point, softness, and high conductivity. Our pure indium wire provides reliable hermetic seals and remains malleable at cryogenic temperatures. Manufactured to meet ASTM B-32, J-STD-006, and JIS-Z-3282 standards, Indium Corporation offers flexible manufacturing for both small and large orders.

Powered by Indium Corporation

  • Low Melting Point Wire
  • High Malleability & Ductility
  • Corrosion Resistant
Five silver wires of varying thicknesses are aligned vertically against a dark green background.

Indium wire has a melting point of 157°C (314°F), significantly lower than many other metals. This low melting point is ideal for applications requiring soft, low-temperature soldering. It also makes Indium suitable for thermal interface applications where heat must be conducted without melting other components.

Indium wire is highly malleable and soft, which allows it to conform to irregular, rough, or non-machined surfaces. Unlike some metals that are hard and brittle, Indium wire is suitable for applications needing a secure fit like gaskets as well as creating airtight seals.

Indium is an excellent conductor of both heat and electricity. It’s particularly useful in electronics, where it’s used to make efficient connections between components. In thermal management, it transfers heat effectively, which is beneficial for heat-sensitive applications.

Indium doesn’t easily oxidize or corrode, even when exposed to environmental factors. This property makes it highly durable for long-term applications in vacuum, cryogenic, and other sealed environments where integrity is crucial.

Dark green icon with stylized shapes and a dot on a white circular background.

Reusability

Dark green icon with stylized shapes and a dot on a white circular background.

Low Outgassing

Dark green icon with stylized shapes and a dot on a white circular background.

Leak Tightness and Reliability

Dark green icon with stylized shapes and a dot on a white circular background.

Non-Toxic and Environmentally Friendly

ParameterDetails
Composition99.99% Pure Indium
Diameter (inches):
≥ 0.010 to ≤ 0.060
≥ 0.060 to ≤ 0.250
≥ 0.060 to ≤ 0.250
Standard Tolerances:
± 0.002
± 0.003
± 2.5%
LengthCustomizable
Temperature Range-200°C to 200°C
Melting Point156.6°C
Surface FinishSmooth, custom finishes available
PackagingSpools and cut to length
PropertyValue
Tensile Strength1.14MPa
Elongation (at break)67%
Density7.31g/cm3
Thermal Conductivity86W/mK
Specific Heat Capacity0.233J/gK

Product Data Sheets

Indalloy®301 for Wire and Bar PDS 100189 R1.pdf

Related Applications

Indium wire is suitable for a wide range of industry applications.

Black textured cylinder with cryogenic seals, featuring three white rectangular labels on top.

Sealing: Cryogenic and Hermetic

Low temperature liquid & fusible alloys for…

Close-up of a computer microchip on a green circuit board with visible electronic components and patterns.

Thermal Management

Thermal solutions for HPC ensuring reliability and…

Close-up of a colorful patterned microchip surface with a grid-like structure and a reflective sheen.

Semiconductor Packaging and Assembly

Critical semiconductor packaging ensures functionality and durability.

Related Markets

Indium Corporation’s indium wire is available for use in a variety of markets.

Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!

This image has an empty alt attribute; its file name is scientist-with-microscope.png

Looking for Safety Data Sheets?

Access everything you need — from technical specifications to application guidance — in one convenient location.