Products Thermal Interface Materials Phase Change Metal TIMs

Phase-Change Metal Alloy (PCMA) TIMs

Metals conduct heat and electricity through their valence electrons, a highly efficient mechanism that applies to both solid and liquid forms of metals and alloys. In addition to their naturally high thermal conductivity, liquid metals also feature low interfacial resistance, enabling them to dissipate heat quickly. Indium Corporation’s PCMA TIMs are engineered to provide exceptional thermal conductivity and reliability, making them ideal for both TIM0 (TIM1.5) and TIM1 applications.

Powered by Indium Corporation

  • High Thermal Conductivity
  • Pure Metal TIMs
  • Liquid Phase During Operational Hours
PCMA thermal aging image

Low Melting Point Metal Alloys

PCMA TIMs are thermal interface materials that are solid at room temperature. With a low melting temperature range (50°C–108°C), they are designed to become liquid or pasty during operation, enhancing heat transfer by filling in surface gaps.

Barrier Material

Since PCMA TIMs will be in a liquid/paste phase during operational hours, there should be a barrier designed that will prevent leakage of those materials.

Thickness Recommendation

The minimum thickness for most alloys is 50 μm, but the recommended thickness for certain applications will depend on the specific warpage of the die (for the semi-conductor applications) and potential CTE mismatch between the surfaces connected with PCMA TIM.

TIM Set Up

If there is any warpage in the package (curved die), it is highly recommended to do a burn-in step with PCMA TIM (70°C for at least 30 seconds). Recommended pressure for PCMA TIMs is between 30 and 40 PSI.

High-Volume Production

Better Volume Control

Avoiding Gallium

Liquid or Pasty

Non-Gallium Containing PCMAs

PCMAPhase Change Temp (°C)Thermal Conductivity (W/mK)Contains Ga?ManufacturabilityOxidationSurface PlanarityReliability
PCMA230560-7218.4NEASYGOODGOODGOOD
PCMA2305+58-6518.4NEASYGREATGOODGOOD
Indalloy® 196019.6NEASYBADBADBAD
PCMA271-7622.6NEASYGOODGOODGOOD
Indalloy® 1627229NEASYOKGOODOK
Indalloy® 1747910NOKOKOKOK
Indalloy® 278112NOKOKOKOK
Indalloy® 22410844NEASYGOODGOODGOOD
Indalloy® 1E11841NEASYGOODGOODGOOD
Indalloy® 28113816NOKOKGOODGOOD
Indalloy® 29014373NEASYGOODGOODGOOD
Indalloy® 415786NEASYGOODGOODGOOD

Related Applications

PCMA TIMs are available for use in a variety of applications.

Close-up of a microchip with a thermal pad layered on top, placed on a circuit board.

Immersion Cooling

A technique on the rise for thermal…

Related Markets

Indium Corporation PCMA TIMs is suitable for a wide range of markets.

Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!

This image has an empty alt attribute; its file name is scientist-with-microscope.png

Looking for Safety Data Sheets?

Access everything you need — from technical specifications to application guidance — in one convenient location.