Products Compounds Gallium Trichloride (EZ-Pour®)

Gallium Trichloride (EZ-Pour®)

Gallium trichloride (GaCl3), also known as gallium chloride, is essential in the MOCVD industry. It’s a key component in creating the gallium precursor Tri-Methyl-Gallium (TMG) for growing GaN layers in CVD processes. Additionally, it’s used in making lithium thionyl chloride (LTC) batteries for oil and gas drilling operations and in producing gallium-based quantum dots like GaP. Indium Corporation offers an exclusive, high-purity, granulated form called EZ-Pour®, known for its safety, integrity, and ease of use.

Powered by Indium Corporation

  • Granulated Form That’s Easy to Pour
  • Extreme Purity
  • Solid GaCl3 Available in Hastelloy Containers
A glass bottle with a red cap containing white granular powder, marked with volume measurements on the side.
PropertyDescription
AppearanceWhite quasi-spherical pellets, deliquescent, fumes in air
Purity99.999% (5N) Standard
Melting Point77.9°C
Boiling Point201.3°C at 760torr
Density• Solid: 2.47g/cm3
• Liquid: 2.05g/cm3 at melting point
• EZ-POUR(R): 1.3-1.4g/cm3
SolubilitySoluble in water, ammonia, benzene, ethers, carbon disulfide, and carbon tetrachloride
101 Tons
Deliquescent
39.6%

Product Data Sheets

EZ-Pour® Granulated Anhydrous Gallium Trichloride PDS 99125 R2.pdf

Related Applications

EZ-Pour® gallium trichloride is available for use in the following applications:

Factory where catalysis is used

Catalysis

Indium and gallium compounds for catalysis, chemical…

Molecular bonds showing chemical synthesis

Chemical Synthesis

Indium and gallium compounds for chemical synthesis…

Related Markets

Indium Corporation’s EZ-Pour® is known for its effective use in many markets.

Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!

This image has an empty alt attribute; its file name is scientist-with-microscope.png

Looking for Safety Data Sheets?

Access everything you need — from technical specifications to application guidance — in one convenient location.