Products Alloys Indalloy®276

Indalloy®276

Indalloy®276 (SnSbAgCu) is a unique lead-free solder alloy engineered for power electronics, offering enhanced reliability and a wide service temperature range up to 175°C.

Powered by Indium Corporation

  • High Reliability
  • Pb-Free
  • Available with InFORMS®, Preforms, Ribbon, Wire, and Paste
Exploded view of an OLED microdisplay with layers separated, showing circuit components and a keypad to the left.

High Reliability at a Wider Service Temperature

Compared to commonly used SAC or SnSb alloys, Indalloy®276 offers consistent solderability in flux-free and conventional reflow applications. When operating temperatures exceed 150°C, Indalloy®276 has achieved superior life-cycle performance.

Pb-Free Technology

With a ROHS-compliant alloy composition, Indalloy®276 is an environmentally-friendly alternative to lead-based solders commonly used in power electronics packaging. With robust mechanical strength and proven reliability performance, Indalloy®276 can be introduced without sacrificing performance for many mission profiles and use case scenarios. 

InFORMS® Complementary Technology

When paired with InFORMS®, Indalloy®276 significantly enhances design reliability. Its robust operating temperature range and reinforced matrix provide greater strength, making Indalloy®276 with InFORMS® the preferred choice for high-power density soldering in power electronics.

Available Configurations

When solder preforms are needed, Indalloy®276 offers a variety of sizes, thicknesses, and standard or custom shapes. Indalloy®276 is also available in ribbon, solder paste, and wire. Preform options include discs, squares/rectangles, washers, frames, and special shapes.

Quick Facts

Robust life cycle performance over a high service temperature range makes Indalloy® 276 the preferred soldering solution in power electronics applications.

175°C
0%

Indalloy®276 Specifications

Selected PropertiesMetric
Liquidus233°C
Solidus224°C
Density7.32g/cc
Thermal Conductivity56W/mk
CTE23ppm/°C
Poisson Ratio0.39
Tensile Strength77MPa
Yield Strength60MPa
Elongation28%

Product Data Sheets

Indium8.9HFRV (869-23-5) High-Reliability Alloy (Indalloy®292 and 276) Solder Paste PDS 99827 R3.pdf
Indium8.9HF High-Reliability (Indalloy®276) Solder Paste PDS 99936 R1.pdf
Indium8.9HF High-Reliability (Indalloy®292 and 276) Solder Paste PDS 99702 R7.pdf
Indium8.9HF (Indalloy®276) Pb-Free Solder Paste PDS 99692 R0.pdf

Related Applications

Indalloy®276 is suitable for a variety of applications.

Close-up of a semiconductor die being precisely soldered by a robotic arm, showcasing advanced die bonding techniques.

Die-Attach

Die-attach solutions include solder pastes to gold-based…

Close-up of a copper electrical component with multiple connectors on a green background.

Clip and Lead Frame Attach

Applications Clip and Lead Frame Attach In…

Exploded view of electronic components on a green background, showing circuit boards, copper connectors, and a central logo.

Package-Attach

Wide selections to address the challenges in…

Spools of thin metal strips and sheets arranged on a grid-patterned surface.

Substrate/Spacer-Attach

Premier substrate-attach solutions in the power module…

Close-up of a colorful patterned microchip surface with a grid-like structure and a reflective sheen.

Semiconductor Packaging and Assembly

Critical semiconductor packaging ensures functionality and durability.

Related Markets

Indalloy®276 is available for use in a wide range of applications.

Looking for Safety Data Sheets?

Access everything you need — from technical specifications to application guidance — in one convenient location.