Gallium is at the foundation of the modern world, powering the semiconductor material without which modern communication technology would be impossible. WiFi, Bluetooth, GPS, and electric vehicles all depend on gallium based semiconductors (GaAs and GaN). To manufacture these semiconductors, metallic gallium is needed to construct the source materials (wafer crystals and epitaxial wafers).

Alimentato da Indium Corporation

  • High Purities Starting at 5N Levels
  • Gallium Shot and Ingot
  • Gallium Compounds and Reclaim Processing Also Available
Primo piano di un cristallo metallico lucido con superfici irregolari e strutturate su uno sfondo verde sfumato.

Gallium melts at just 29.8°C, remaining liquid near room temperature. When alloyed with indium and tin, its melting point is further reduced.

Gallium is being explored for new uses, including medical applications due to its antibiotic properties.

Purity is critical in semiconductor and electronic applications, as impurities can affect electronic and thermal properties. Our gallium typically starts at 5N purity.

Gallium is a byproduct of bauxite (aluminum) production. While global supply diversity has decreased, we are working to enhance the supply chain.

Dark green icon with stylized shapes and a dot on a white circular background.

Gallium Semiconductors

Dark green icon with stylized shapes and a dot on a white circular background.

Bauxite, Zinc Ore, Fly Ash

Dark green icon with stylized shapes and a dot on a white circular background.

MOCVD

Dark green icon with stylized shapes and a dot on a white circular background.

Solar Applications

Applicazioni correlate

High-purity gallium is a necessary product for a wide-range of applications due to its unique properties.

Primo piano di un microchip per computer su un circuito verde con componenti elettronici e modelli visibili.

Gestione termica

Soluzioni termiche per l'HPC che garantiscono affidabilità e…

Legami molecolari che mostrano la sintesi chimica

Sintesi chimica

Composti di indio e gallio per la sintesi chimica…

Fabbrica in cui viene utilizzata la catalisi

Catalisi

Composti di indio e gallio per la catalisi, la chimica…

Mercati correlati

High-purity gallium is essential in the Compound Semiconductor and Batteries industries. Many industries downstream from these use high-purity gallium components and devices.

Avete domande tecniche o richieste di vendita? Il nostro team dedicato è qui per aiutarvi. "Da un ingegnere all'altro®" non è solo il nostro motto: è il nostro impegno a fornire un servizio eccezionale. Siamo pronti quando lo siete voi. Mettiamoci in contatto!

Questa immagine ha un attributo alt vuoto; il suo nome file è scientist-with-microscope.png

Cercate le schede di sicurezza?

Accedete a tutto ciò che vi serve, dalle specifiche tecniche alle indicazioni per le applicazioni, in un'unica comoda posizione.