Indium Corporation has released TACFlux 571HF, a new no-clean, halogen-free flux formulated for both hand soldering and rework.
TACFlux 571HF joins Indium Corporations versatile offering of specialty fluxes designed to provide solutions for current and evolving industry challenges. Compatible with typical Pb-free (SAC), as well as low-temp bismuth- and indium-containing alloys for PCB assembly applications, benefits include:
- Halogen-free per IEC 61249-2-21 test method EN14582
- Clear post-reflow flux residue for no-clean applications
- Shelf life of up to 1 year
For more information about TACFlux 571HF, visit https://www.indium.com/products/fluxes/.
About Indium Corporation
Indium Corporation is a premier materials refiner, smelter, manufacturer, and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil. Founded in 1934, the company has global technical support and factories located in China, Germany, India, Malaysia, Singapore, South Korea, the United Kingdom, and the U.S.
For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email Jingya Huang. You can also follow our experts, From One Engineer To Another (#FOETA), at www.linkedin.com/company/indium-corporation/ or @IndiumCorp.