Indalloy®276 (SnSbAgCu) is a unique lead-free solder alloy engineered for power electronics, offering enhanced reliability and a wide service temperature range up to 175°C.
Powered by Indium Corporation
- High Reliability
- Pb-Free
- Available with InFORMS®, Preforms, Ribbon, Wire, and Paste
Product Overview
High Reliability at a Wider Service Temperature
Compared to commonly used SAC or SnSb alloys, Indalloy®276 offers consistent solderability in flux-free and conventional reflow applications. When operating temperatures exceed 150°C, Indalloy®276 has achieved superior life-cycle performance.
Pb-Free Technology
With a ROHS-compliant alloy composition, Indalloy®276 is an environmentally-friendly alternative to lead-based solders commonly used in power electronics packaging. With robust mechanical strength and proven reliability performance, Indalloy®276 can be introduced without sacrificing performance for many mission profiles and use case scenarios.
InFORMS® Complementary Technology
When paired with InFORMS®, Indalloy®276 significantly enhances design reliability. Its robust operating temperature range and reinforced matrix provide greater strength, making Indalloy®276 with InFORMS® the preferred choice for high-power density soldering in power electronics.
Available Configurations
When solder preforms are needed, Indalloy®276 offers a variety of sizes, thicknesses, and standard or custom shapes. Indalloy®276 is also available in ribbon, solder paste, and wire. Preform options include discs, squares/rectangles, washers, frames, and special shapes.
Quick Facts
Robust life cycle performance over a high service temperature range makes Indalloy® 276 the preferred soldering solution in power electronics applications.
Indalloy®276 Specifications
| Selected Properties | Metric |
|---|---|
| Liquidus | 233°C |
| Solidus | 224°C |
| Density | 7.32 g/cc |
| Thermal Conductivity | 56 W/mk |
| CTE | 23 ppm/°C |
| Poisson Ratio | 0.39 |
| Tensile Strength | 77 MPa |
| Yield Strength | 60 MPa |
| Elongation | 28% |
Product Data Sheets
Indium8.9HFRV (869-23-5) High-Reliability Alloy (Indalloy®292 and 276) Solder Paste PDS 99827 R3.pdf
Indium8.9HF High-Reliability (Indalloy®276) Solder Paste PDS 99936 R1.pdf
Indium8.9HF High-Reliability (Indalloy®292 and 276) Solder Paste PDS 99702 R7.pdf
Indium8.9HF (Indalloy®276) Pb-Free Solder Paste PDS 99692 R0.pdf
Related Applications
Indalloy®276 is suitable for a variety of applications.
Related Markets
Indalloy®276 is available for use in a wide range of applications.
Expert Support for Reliable Results
Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!
Looking for Safety Data Sheets?
Access everything you need — from technical specifications to application guidance — in one convenient location.
Your Success
is Our Goal
Optimize your processes with the latest materials, technology, and expert application support. It all starts by connecting with our team.