Products Compounds Gallium Acetylacetonate

Gallium Acetylacetonate

Gallium acetylacetonate (Ga(acac)3) is an organic compound. Technically, it represents an organometallic coordination complex with gallium at the center, surrounded by three acetylacetonate ligands. When heated in the presence of oxygen, gallium acetylacetonate decomposes into gallium oxide (Ga2O3). This property makes Ga(acac)3 a useful precursor for growing highly pure and uniform Ga2O3 thin films on substrates such as glass and silicon. Ga(acac)3 is used in the production of quantum dots like Ga2S3, GaAs, GaP, and GaInP.

Powered by Indium Corporation

  • Thermally Stable and Decomposes at Higher Temperatures Compared to TMG
  • Ga(acac)3 Is Not Pyrophoric Like TMG, Making It Safer to Handle
  • Soluble in Organic Solvents
Two mounds of white powder, possibly acetylacetonate, rest on a smooth, light-colored surface.
PropertyValue
Chemical FormulaGa(C₅H₇O₂)₃
Molecular Weight367.05g/mol
Density (Bulk)1.42g/cm³
Melting Point196–198°C
Crystal StructureMonoclinic
Purity4N (99.99%)
Gallium Content (Theoretical)19%
SolubilitySoluble in organic solvents, insoluble in water
Dark green icon with stylized shapes and a dot on a white circular background.

19%

Dark green icon with stylized shapes and a dot on a white circular background.

Monoclinic

Dark green icon with stylized shapes and a dot on a white circular background.

300°C

Dark green icon with stylized shapes and a dot on a white circular background.

3.3 eV

Product Data Sheets

Gallium Acetylacetonate PDS 100109 R0.pdf

Related Applications

Ga(acac)3 is suitable for a variety of applications.

Molecular bonds showing chemical synthesis

Chemical Synthesis

Indium and gallium compounds for chemical synthesis…

Three metallic indium bars with reflective surfaces placed on a dark background.

Thermal Evaporation and PVD Coating

Achieve efficient and high-quality thin film deposition.

Related Markets

Ga(acac)3, produced by Indium Corporation, is available for use in a variety of markets.

Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!

This image has an empty alt attribute; its file name is scientist-with-microscope.png

Looking for Safety Data Sheets?

Access everything you need — from technical specifications to application guidance — in one convenient location.