Indium Corporation has added to its line of thermal interface materials (TIMs) with the introduction of HSMF-OS, a non-silicone based metal/polymer material designed for burn-in and test applications.
HSMF-OS is designed for high insertion capability. Its high tensile strength and soft compliant polymer backing allow it to survive multiple insertions. HSMF-OS has been tested to withstand over 5,000 insertion cycles without any loss of performance.
One of the challenges associated with a burn-in TIM is the attachment method. HSMF-OS has inherent adhesive properties on one side that allow for hand placement, removing the need for these additional steps and fixtures without compromising thermal performance. The opposite side is aluminum and it will not mark or stain the DUI (device under test).
HSMF-OS offers consistently good performance without phase change.
For more information on HSMF-OS and Indium Corporation’s full line of TIMs, visit indiumstg.wpenginepowered.com/TIMs.
Indium Corporation è uno dei principali produttori e fornitori di materiali per i mercati globali dell'elettronica, dei semiconduttori, dei film sottili e della gestione termica. I prodotti includono saldature e flussanti, brasature, materiali per interfacce termiche, target per sputtering, metalli e composti inorganici di indio, gallio, germanio e stagno e NanoFoil®. Fondata nel 1934, l'azienda dispone di un'assistenza tecnica globale e di stabilimenti situati in Cina, Malesia, Singapore, Corea del Sud, Regno Unito e Stati Uniti.
Per ulteriori informazioni su Indium Corporation, visitate il sitoindiumstg.wpenginepowered.como inviate un’e-mailall’indirizzo [email protected]. Potete inoltre seguire i nostri esperti, From One Engineer ToAnother®(#FOETA), suwww.facebook.com/indiumo su@IndiumCorp.