Indium Corporation will feature its Indium8.9HF Solder Paste at Productronica India, September 25-27, in Greater Noida, Delhi National Capital Region, India.
Indium8.9HF is a proven solder paste series that delivers no-clean, halogen-free solutions designed to produce low-voiding, enhanced electrical reliability, and improved stability during the printing process. Under optimal process conditions, Indium8.9HF:
- Demonstrates consistent printing performance for up to 12 months when refrigerated
- Maintains excellent printing and reflow performance after remaining at room temperature for one month
- Delivers excellent response-to-pause, even after being left on the stencil for 60 hours
- Resists premature flux spread to prevent surfaces from oxidizing
- Performs with both Pb and Pb-free alloys
For information on Indium8.9HF, visit Indium Corporation booth #PD41 at the show, or indiumstg.wpenginepowered.com/avoidthevoid.
Indium Corporation is a premier materials manufacturer and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, the company has global technical support and factories located in China, India, Malaysia, Singapore, South Korea, the United Kingdom, and the USA.