Products Compounds Indium Sulfamate Plating Bath

Indium Sulfamate Plating Bath

Enhance your plating process with our indium sulfamate plating bath, designed to deposit high-purity indium on a variety of substrates. Whether you’re working on prototypes or large-scale production, this premium solution delivers the performance and reliability essential for industries like microelectronics and aerospace, ensuring top-quality metal finishes every time.

Powered by Indium Corporation

  • Exceptional Stability
  • Uniform Deposition
  • High-Throwing Formulation
A clear 1-liter chemical bottle with a warning label is placed upright. Two silver metal strips lie beside it on a black surface.

Indium Corporation’s sulfamate electroplating solution is available in small bottles, 55-gallon drums, or larger totes, providing flexibility to suit any production scale. This room-temperature plating bath requires minimal additives, in large part due to its efficient anode system that continuously replenishes indium metal. With proper maintenance, the bath can last for years, requiring only occasional solution top-ups.

The plating can be applied to a range of well-prepared substrate metallizations, including copper, brass, nickel, gold, tin, and mild steel. However, stainless steel and aluminum require specialized surface treatments before electroplating with any metal.

  • Indium content: 30g/L and above, depending on specific requirements
  • pH range: 1.5–3.5 (preferred 1.5–2.0)
  • Operating temperature: Room temperature (20-25°C)
  • Cathode efficiency: 90%
  • Anode efficiency: 100%
  • Deposition rate: Approx. 1.5 mils/hour at 20amps/ft²
Dark green icon with stylized shapes and a dot on a white circular background.

Pioneering Excellence

Dark green icon with stylized shapes and a dot on a white circular background.

Green and Clean

Dark green icon with stylized shapes and a dot on a white circular background.

Optimal Performance

Dark green icon with stylized shapes and a dot on a white circular background.

Cathodic Efficiency

Prepared as a ready-to-use solution with a standard concentration of 30g/l of indium ions with tailoring options to meet specific customer requirements.

A comprehensive electroplating kit ideal for small-scale electroplating projects and prototype construction. The kit includes:

  • 1 liter of sulfamate plating bath solution
  • Two thin indium metal strips (1” x 12” x 0.0625″, 4N purity) as anode material
  • A plating manual detailing the setup, operation, and maintenance of an indium plating bath

Product Data Sheets

Indium Sulfamate Plating Bath PDS 97686 R5.pdf

Related Applications

Indium sulfamate plating baths are suitable for a variety of applications.

Metal frames being treated with an electroplating kit in a factory setting with several tanks.

Electroplating

Try indium electroplating to enhance appearance and…

Close-up of a square semiconductor chip with four subdivided sections on a green and black background.

Flip-Chip

A crucial technique in advanced semiconductor packaging.

A grid of evenly spaced, smooth, spherical particles on a black background.

Bump Fusion

Achieve robust solder bumps on wafers with…

Related Markets

Indium Corporation’s indium sulfamate plating baths are recommended for use in the following markets:

Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!

This image has an empty alt attribute; its file name is scientist-with-microscope.png

Looking for Safety Data Sheets?

Access everything you need — from technical specifications to application guidance — in one convenient location.