In celebration of Indium Corporation’s 85th anniversary, the company will release monthly installments of the Elements of Indium Series—an educational program to raise awareness of the unique applications, abundance, and interesting properties of the 49th element.
Indium Corporation is the global leader for indium metal and associated technologies. Because of its unique properties with virtually limitless applications, indium metal is literally all around us.
Not many metals have the ability to performs in harsh low-temperature environments like indium metal can. Traditional metals containing Sn or Pb fail at cryogenic temperatures (<-180°C). Because indium deforms indefinitely under pressure, cryogenic seals made from indium won’t crack or leak in aerospace and other cold, high-vacuum environments.
For more information on indium metal, visit indiumstg.wpenginepowered.com/indium49.
Indium Corporation is a premier materials manufacturer and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, the company has global technical support and factories located in China, India, Malaysia, Singapore, South Korea, the United Kingdom, and the USA.
For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email [email protected]. You can also follow our experts, From One Engineer To Another®(#FOETA), at www.facebook.com/indium or @IndiumCorp.