Indium Corporation Announces Ultrafine 0.006″ (0.15mm) Flux-Cored Wire Capabilities

Indium Corporation announces that it is now offering ultrafine flux-cored wire down to 0.006” (0.15mm) in diameter for standard Pb-free alloys.

Indium Corporation’s ultrafine flux-cored wire was developed to meet the progressively demanding requirements for increased solder joint density and miniaturization in applications where solder paste reflow and other soldering approaches are not effective, such as robotic soldering, fine-pitch component attachment, and hand soldering. Indium Corporation flux-cored wire offers:

  • Evenly wound layers onto the spools to avoid tangles during use
  • Consistent diameters that meet the most stringent requirements
  • No flux voids within the wire for consistent, worry-free soldering

Indium Corporation uses only “conflict-free” and grade A (per ASTM B32) metals, as well as other high-purity metals for its flux-cored wire. All materials have been tested and certified to meet IPC J-STD-004B and other relevant industry specifications, including the legacy military specification QQ-S-571F.

Featured flux vehicles for the 0.006” wire is Core 230-RC (REL1) and CW-808 (REL0). Both of these fluxes were developed for robotic soldering applications and contain Indium Corporation’s low-spatter technology.

For more information, visit https://www.indium.com/flux-and-epoxy/flux-cored-wire/ or contact Robert McKerrow, Product Specialist – Flux-Cored Wire, Wave Solder Flux, and Bar Solder, at [email protected].

Indium Corporation est un fabricant et fournisseur de matériaux de premier plan sur les marchés mondiaux de l'électronique, des semi-conducteurs, des couches minces et de la gestion thermique. Ses produits comprennent des soudures et des flux, des brasures, des matériaux d'interface thermique, des cibles de pulvérisation, des métaux et des composés inorganiques à base d'indium, de gallium, de germanium et d'étain, ainsi que des NanoFoil®. Fondée en 1934, l'entreprise dispose d'une assistance technique mondiale et d'usines situées en Chine, en Malaisie, à Singapour, en Corée du Sud, au Royaume-Uni et aux États-Unis.

Pour plus d'informations sur Indium Corporation, rendez-vous surindiumstg.wpenginepowered.comou envoyez un e-mailà [email protected]. Vous pouvez également suivre nos experts, « From One Engineer ToAnother® »(#FOETA), surwww.facebook.com/indiumou@IndiumCorp.