Indium Corporation Announces New Solder Paste Technology

Indium Corporation announces a new solder paste technology. BiAgX® is a high-melting lead-free (Pb-free) solder paste technology designed for high reliability electronics assembly applications. Designed as a drop-in replacement for standard high Pb-containing solder pastes, it has passed MSL1 and thermal cycle testing at several power semiconductor customers.

BiAgX® is excellent for small, low-voltage QFN packages that are used in portable electronics (smartphone/tablet), automotive electronics, and industrial applications. It excels in high temperature environments in excess of 150°C. It requires minimal process adjustments and no capital expenditures for customers converting from a standard high Pb-containing solder paste-based process.

BiAgX® addresses both customer demands and potential legislative changes that eliminate lead from high-melting die-attach applications. It is both Pb-free and Sb-free (lead and antimony) and does not contain costly specialty materials, such as nanosilver or sintering aids.

BiAgX® reflows, solders, wets, and solidifies just like any other solder paste, and is available in both dispense and printing forms. Fluxes are cleanable with standard cleaning chemistries and processes.

For more information about BiAgX®, including technical papers and other technical information, visit indiumstg.wpenginepowered.com/BiAgX.

Indium Corporation è uno dei principali produttori e fornitori di materiali per i mercati globali dell'elettronica, dei semiconduttori, del solare, dei film sottili e della gestione termica. I prodotti includono saldature, preforme e flussanti; brasature; bersagli per sputtering; metalli e composti inorganici di indio, gallio e germanio e NanoFoil®. Fondata nel 1934, Indium dispone di un'assistenza tecnica globale e di stabilimenti situati in Cina, Singapore, Corea del Sud, Regno Unito e Stati Uniti.

Per ulteriori informazioni su Indium Corporation, visitate il sito indiumstg.wpenginepowered.com o inviate un’e-mail all’indirizzo [email protected].