Vai al contenuto

Indium Corporation’s New Indium10.8HF Solder Paste Technology Exhibits Best-in-Class Non-Wet Open Performance

Indium Corporation's new Indium10.8HF is a halogen-free, no-clean solder paste that is formulated to provide industry-leading non-wet open performance on large, high IO electronic packages, such as microprocessors.   

In addition to its resistance to non-wet opens, Indium10.8HF also delivers a superior oxidation barrier, allowing for reduced head-in-pillow (HiP) defects and improved graping performance. It also exhibits exceptional stencil printing, especially for small components (01005) and fast printing speeds (>125 mm/sec).

Indium10.8HF solder paste is part of Indium Corporation's family of high-performance, lead-free, low-voiding, no-clean solder pastes that help manufacturers Avoid the Void™. For more information about Indium10.8HF, email [email protected] or visit indiumstg.wpenginepowered.com/indium10.8HF.

Indium Corporation è uno dei principali produttori e fornitori di materiali per i mercati globali dell'elettronica, dei semiconduttori, dei film sottili, della gestione termica e del solare. I prodotti includono saldature e flussanti, brasature, materiali per interfacce termiche, bersagli per sputtering, metalli e composti inorganici di indio, gallio, germanio e stagno e NanoFoil®. Fondata nel 1934, Indium dispone di un'assistenza tecnica globale e di stabilimenti situati in Cina, Malesia, Singapore, Corea del Sud, Regno Unito e Stati Uniti.

Per ulteriori informazioni su Indium Corporation, visitate il sitoindiumstg.wpenginepowered.como inviate un’e-mailall’indirizzo [email protected]. Potete inoltre seguire i nostri esperti, From One Engineer ToAnother®(#FOETA), suwww.facebook.com/indiumo su@IndiumCorp.