Indium Corporation Experts to Present on Solder and Thermal Solutions at APEX 2025

As a global supplier of solder and thermal interface material (TIM) products, Indium Corporation experts are proud to share their technical insight and knowledge on a variety of industry-related topics at IPC APEX Expo, March 18-20 in Anaheim, California. 

Tuesday, March 18 

  • Achieving Lower Voids with a Novel Preform Flux Technology, presented by Research Chemist David Bedner, and co-authored by Lee Kresge, Igor Faleichik, Dan McElhinney, and Dr. Ricky McDonough. 
  • This presentation introduces a next-generation preform flux that significantly reduces voiding in solder joints, enhancing thermal performance and reliability across various applications, with testing demonstrating up to a 67% reduction in voids under optimized reflow conditions. 

Wednesday, March 19 

  • This presentation explores the development of novel mixed-alloy solder paste Durafuse® HR, which reduces voiding while maintaining high-reliability thermal cycling performance, offering improved solutions for automotive, high-performance computing, and 5G communication applications. 
  • Novel Supercooled Solder Materials for Lower-Than-Liquidus Reflow presented by R&D Manager Dr. Ian Tevis, co-authored by Dr. Yifan Wu and Radhika Jadhav. 
  • This presentation showcases the development of supercooled solder pastes using core-shell bismuth-tin (BiSn) particles, enabling reliable solder interconnects at temperatures 40°C lower than conventional reflow profiles, making them ideal for future electronics manufacturing and temperature-sensitive applications. 
  • Liquid Metal Paste High-Speed Dispensing for High-Volume Manufacturing – Part II, co-presented by Senior Product Specialist Miloš Lazić and Sunny Agarwal, ITW EAE. Co-authored by Dr. Ricky McDonough. 
  • This presentation examines the advancements in liquid metal paste (LMP) technology, showcasing its enhanced thermal conductivity and adaptability for high-performance computing applications, while addressing challenges associated with traditional liquid metal thermal interface materials (TIMs). 
  • This presentation introduces newly developed gallium-based and gallium-free phase-change metal (PCM) TIMs, designed to remain in a liquid state at operating temperature, delivering exceptionally low thermal resistance. Power cycling and HAST data highlight their robust performance and underscore the necessity of containment strategies, while gallium-free solutions enable compatibility with aluminum heat-sinks. 

To learn more about Indium Corporation’s solder and TIMs solutions, visit indiumstg.wpenginepowered.com or visit with our experts at APEX 2025 in booth #1416. 

About Indium Corporation 

IndiumCorporation® est l'un des principaux raffineurs, fondeurs, fabricants et fournisseurs de matériaux destinés aux marchés mondiaux de l'électronique, des semi-conducteurs, des couches minces et de la gestion thermique. Sa gamme de produits comprend des soudures et des flux ; des alliages de brasage ; des matériaux d'interface thermique ; des cibles de pulvérisation ; de l'indium, du gallium, du germanium et de l'étain sous forme de métaux et de composés inorganiques ; ainsi quele NanoFoil®. Fondée en 1934, la société dispose d'un service d'assistance technique mondial et d'usines situées en Chine, en Allemagne, en Inde, en Malaisie, à Singapour, en Corée du Sud, au Royaume-Uni et aux États-Unis. 