Indium Corporation’s Aaron Yan, Area Technical Manager – Eastern China, will present at the IPC Shanghai Technology Seminar on July 17 in Shanghai, China.
Yan’s presentation, High-Temperature Lead-free BiAgX® Material, will discuss BiAgX – a high-melting, lead-free (Pb-free) solder paste technology that is a drop-in replacement for high-Pb solders used in many high-reliability die-attach and electronics assembly applications. Yan will also address how BiAgX is suited for small, low-voltage QFN packages that are used in portable electronics (smartphones/tablets), automotive electronics, and industrial applications.
Yan is responsible for providing technical support for Indium Corporation's electronics assembly materials, semiconductor and advanced assembly materials, engineered solders, and thermal management materials. Yan has more than 12 years of experience in surface mount technology, specializing in defect prevention, continuous quality improvement, and cost reduction.
IPC is a global trade association dedicated to furthering the competitive excellence and financial success of its electronics industry members. For more information about upcoming presentations, visit www.ipc.org.cn/Events/Technology-Seminar/2015.
Indium Corporation is a premier materials manufacturer and supplier to the global electronics, semiconductor, solar, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, Indium has global technical support and factories located in China, Malaysia, Singapore, South Korea, the United Kingdom, and the USA.
For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email [email protected]. You can also follow our experts, From One Engineer To Another® (#FOETA), at www.facebook.com/indium or @IndiumCorp.