Indium Corporation to Feature Precision Au-Based Die-Attach Preforms at SPIE Photonics West

Indium Corporation will feature its high-reliability, Au-based precision die-attach (PDA) preforms for critical laser and RF applications at SPIE Photonics West, Jan. 27-Feb. 1, in San Francisco. SPIE West is the world’s premier event for lasers, biomedical optics and biophotonic technologies, quantum, and optoelectronics. 

Indium Corporation is the leading solder supplier for laser and optical applications. Au-based alloys are a great choice to ensure the best performance and reliability possible for applications requiring a high-melting die-attach solder. In addition to meeting the demanding thermal and electrical requirements for high-reliability applications, they also provide the strongest corrosion- and oxidation-resistant solder joint possible. 

Semiconductor laser die-attach applications require the highest quality, ultra-precise solder preforms to ensure accuracy and repeatability during assembly for a guaranteed highly reliable end product. Indium Corporation’s Au-based PDA preforms offer the NEW Gold Standard – the highest level of quality available to deliver the best performance possible in critical, high-reliability die-attach applications. Features include:

  • Highly accurate thickness control
  • Precise edge quality
  • Optimized cleanliness
  • Default waffle pack method
  • Available for gold-based alloys

Indium Corporation’s AuLTRA 75 is an off-eutectic AuSn preform solution (75Au/25Sn) designed to improve intermetallic reliability in applications using a die with a thicker gold plating, such as a GaN die used for high-frequency, high-power RF power amplifier devices for 5G and other critical military and aerospace wireless communications. AuLTRA 75 helps improve the operation of these critical technologies by adjusting the final solder joint composition and improving wetting and voiding. The AuLTRA product line also comes in 78Au/22Sn and 79Au/21Sn compositions. 

Indium Corporation’s AuLTRA ThInFORMS are 0.00035″-thick (0.00889mm or 8.89m) 80Au/20Sn preforms that improve the overall operational efficiency of high-output lasers. AuLTRA ThInFORMS help combat common issues such as:

  • Shortingreduced solder volume inhibits wicking up the die, minimizing the risk of shorting
  • Poor thermal transferthe ultra-thin 0.00035″ preform reduces bondline thickness (BLT), thus improving thermal transfer and increasing the longevity and performance of the device.

A leading gold solder innovator, Indium Corporation’s gold-based portfolio includes wire, paste, preforms, spheres, shot, and ribbon manufactured with cutting-edge technology to ensure supreme quality and the utmost precision. The most commonly used gold-based alloy is 80Au/20Sn; it is the pillar alloy of the microelectronics industry with a melting point of 280C and works exceptionally well in the majority of die-attach and lid sealing applications. It exhibits good thermal fatigue properties and is used in many applications that require high tensile strength and high corrosive resistance. Indium Corporation’s AuSn solder offers numerous benefits including:

  • Highest tensile strength of any solder
  • High melting point compatible with subsequent reflow processes
  • Superior thermal conductivity
  • Resistance to corrosion 

Additionally, Heat-Spring  is a compressible, non-reflow metal TIM ideal for TIM2 applications. These indium-containing TIMs offer superior thermal conductivity over non-metalswith pure indium metal delivering 86W/mK in all planes. Because of its sold metal state, Heat-Spring avoids pump-out and bake-out problems. It also offers a sustainable solution due to our indium reclaim and recycle program.

To learn more about Indium Corporation’s precision Au-based preforms, visit indiumstg.wpenginepowered.com/products/solders/gold/gold-preforms or stop by booth #5017 at the show. 

About Indium Corporation

Indium Corporation is a premier materials refiner, smelter, manufacturer, and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil. Founded in 1934, the company has global technical support and factories located in China, Germany, India, Malaysia, Singapore, South Korea, the United Kingdom, and the U.S.