One of the most highly demanded applications for 80Au/20Sn is semiconductor laser die-attach due to recent advancements that have made lasers an economical option for a multitude of new products. However, a key challenge with semiconductor lasers is thermal management, as these devices generate a significant amount of heat. Indium Corporation Product Specialist Jenny Gallery will present on how to manage heat with AuSn preforms at the International Microwave Symposium, Denver, Colo., June 1924.
One method for facilitating thermal transfer from the die to the substrate is to reduce the bondline thickness through the use of thinner 80Au/20Sn preforms. By using a thinner preform in the bondline, the heat is transferred away from the die more quickly, increasing the longevity and potential of the die. In The Effect of Semiconductor Laser Thermal Transfer in Relation to AuSn Preform Thickness, Gallery will examine the impact of AuSn preform thickness on thermal transfer by examining voiding percentages on several 80Au/20Sn preforms ranging from 0.002 to 0.00035 thick.
Gallery is a product specialist for the high-temperature business (gold and braze products) at Indium Corporation. She is responsible for researching and analyzing customer and market data, and she serves as a resource to the companys current and prospective customers, field sales, and internal departments. She provides product and process support for solder preforms, wire, ribbon, and paste, and she helps to facilitate relationships and new business development. Gallery earned her bachelors degree in chemistry at the University of Albany, N.Y., U.S.
인디엄 코퍼레이션 소개
Indium Corporation 은 전 세계 전자, 반도체, 박막 및 열 관리 시장에 최고의 소재 정제, 제련, 제조 및 공급업체입니다. 제품에는 솔더 및 플럭스, 브레이즈, 열 인터페이스 재료, 스퍼터링 타겟, 인듐, 갈륨, 게르마늄, 주석 금속 및 무기 화합물, NanoFoil 이 포함됩니다. 1934년에 설립된 이 회사는 중국, 독일, 인도, 말레이시아, 싱가포르, 한국, 영국, 미국에 글로벌 기술 지원 및 공장을 보유하고 있습니다.
인디움 코퍼레이션에 대한 자세한 정보는 www.indium.com 또는 징야 황에게 이메일을 보내주세요. 또한 From One Engineer To Another (#FOETA)의 전문가를 www.linkedin.com/company/indium-corporation/ 또는 @IndiumCorp에서 팔로우할 수도 있습니다.
국제 마이크로파 심포지엄 정보
For 70 years, IMS has brought together a unique mix of international RF and microwave experts presenting the latest research and showcasing the new products and services. IMS includes education and networking opportunities as well as an exhibition. Learn more at ims-ieee.org.