Indium Corporation will feature its reinforced solder alloy fabrications, InFORMS®, at APEC 2017, March 26-30, in Tampa, Fla.
InFORMS are reinforced solder preforms that increase lateral strength and stability. As a result, improved thermal cycling reliability can be achieved.
In one study where InFORMS were used to solder a DBC to the baseplate of an IGBT, the following were achieved:
- Fiabilité des cycles thermiques améliorée de 4x par rapport à une approche basée uniquement sur la préforme de soudure
- Fiabilité des cycles thermiques multipliée par deux par rapport à l'approche préforme de soudure + suture par fil d'aluminium
- Low-voiding of <1%
- Lower cost of ownership – an InFORM is a drop-in replacement for a standard preform or solder paste, requiring no additional process steps or equipment
For more information about InFORMS, visit indiumstg.wpenginepowered.com/informs or visit Indium Corporation at booth #525.
Pour plus d'informations sur Indium Corporation, rendez-vous surindiumstg.wpenginepowered.comou envoyez un e-mailà [email protected]. Vous pouvez également suivre nos experts, « From One Engineer ToAnother® »(#FOETA), surwww.facebook.com/indiumou@IndiumCorp.