Indium Corporation introduces a new Pb-free solder paste designed to combine best-in-class stencil printing performance, using Indiums unique halogen-free oxidation barrier technology with optimized no-clean residues for enhanced probe testing. Indium8.9HF1-P saves time and money on testing by eliminating false failures and giving the highest first pass yields.
Indium8.9HF1-P has proven low cost-of-ownership for PCB assemblies, said Tim Jensen, Global Product Manager for Indium Corporations PCB assembly products. Our customers have been asking for a high-performance solder paste that combines excellent printability with probe-testability. This solder paste delivers on all counts. What this means is that Indium8.9HF1-P will deliver long-term reliability for our customers end products.
Indium8.9HF1-P provides high transfer efficiency, and consistent print performance, even at high speeds. Additionally this paste has a robust response-to-pause, lessening the need for frequent under-stencil wiping. Indium8.9HF1-P prints well on apertures with area ratios <0.5, using low print pressures. Indium Corporations unique oxidation barrier technology enhances reflow performance, eliminating defects such as head-in-pillow and graping.
Indium8.9HF1-P is optimized for probe-testability in two ways: it has a soft residue after reflow, which is easily penetrable by test probes, and this residue remains probe-testable after multiple reflows, time between reflow and test, and baking.
Indium Corporation est un fabricant et fournisseur de matériaux de premier plan sur les marchés mondiaux de l'électronique, des semi-conducteurs, de l'énergie solaire, des couches minces et de la gestion thermique. Ses produits comprennent des soudures, des préformes et des flux, des brasures, des cibles de pulvérisation, des métaux et des composés inorganiques à base d'indium, de gallium et de germanium, ainsi que des feuilles NanoFoil®. Fondée en 1934, Indium dispose d'une assistance technique mondiale et d'usines situées en Chine, à Singapour, en Corée du Sud, au Royaume-Uni et aux États-Unis.
Pour plus d'informations sur Indium Corporation, rendez-vous sur indiumstg.wpenginepowered.com ou envoyez un e-mail à [email protected].