Indium Corporation will co-host a seminar with Process Lab.Micron on Advanced Void-Reducing Technologies for Infrastructure and Communications on Aug. 24 in Shanghai.
The seminar will include an introduction to Indium Corporation's latest halogen-free, Pb-free, no-clean, low-voiding solder paste technology, Indium10.1HF, by Dr. Ning-Cheng Lee and Mary Ma.
Technical experts will lead discussions on:
- InFORMS® and Solder Preforms in Electronics Assembly by Sunny Neoh Soon Chye
- DFX on High-Density Assembly by Wisdom Qu
- Semiconductor Materials for Infrastructure and Communications by Aaron Yan
Dr. Ning-Cheng Lee, Indium Corporation Vice President of Technology, will provide a session focusing on:
- Low temperature solders
- High-reliability solder alloy for wide service temperature capability
- Pressureless Ag/Cu sintering paste
For more information or to register for this seminar, contact [email protected].
Indium Corporation is a premier materials manufacturer and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil®. Founded in 1934, Indium has global technical support and factories located in China, Malaysia, Singapore, South Korea, the United Kingdom, and the USA.
Process Lab.Micron Co., Ltd. is a stencil manufacturer known for developing numerous groundbreaking technologies, such as additive and laser-cut stencils, which have become well established in the stencil industry. The company develops, manufactures, and sells metal masks for electronics component mounting, and precision versions for semiconductor packages and display masks. Process Lab.Micron also performs precision machining and prototyping by etching, plating, and laser cutting. For more information on Process Lab.Micron, visit www.lab-micron.co.jp.
For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email [email protected]. You can also follow our experts, From One Engineer To Another® (#FOETA), at www.facebook.com/indium or @IndiumCorp.