Semiconductor Solder Pastes
Fine Powder Solder Pastes
Indium Corporation’s fine powder solder pastes are expertly designed to address the growing demands of miniaturization in the electronics industry. Suitable for a variety of applications, including printing, contact dispensing, and jetting, these pastes are specifically formulated to cater to unique customer requirements. Special attention during flux and powder production ensures that the final product is optimized to effectively tackle manufacturing challenges and increase yields.
Powered by Indium Corporation
- High-Quality Powder for High Yield
- Excellent Wetting on Various Substrates
- Covers Printing, Jetting, and Dispensing
Product Overview
Excellent Powder Manufacturability
Indium Corporation’s fine solder powders (Type 6, Type 7, and Type 8) are produced with a particle size distribution that meets IPC standards, ensuring minimal fines and excess particles. Special care during the manufacturing process optimizes the powder’s smoothness and sphericity, resulting in high production yields and minimal defects—particularly on thin substrates that are prone to warpage.
Excellent Flux Capability
The flux used in our fine-powder solder pastes undergo additional proprietary manufacturing steps to ensure high production yields in advanced packaging. This includes the elimination of fine flux impurities that could disrupt the printing process, as well as the inclusion of robust oxidation barriers to prevent further oxidation of the solder powder.
Quick Facts
Fine Powder Solder Pastes Products
- Applied by printing or jetting
- Reflow in inert atmosphere (typically <100 ppm 02 level)
- Compatible with SnAgCu, SnAg, SnSb, or other common Pb-free alloys
- Available in Type 5, Type 6, Type 7, and Type 8 powder size for fine-feature applications
| Flux Type* | Flux Application Method | Description | Cleaning Method | Halogen-Free | Material |
|---|---|---|---|---|---|
| WS | Printing | Best all-around pure water-soluble paste | Warm DI water | Yes | SiPaste® 3.2HF |
| C | Printing | Good wetting power and HIP mitigation | DI water + saponifier or semi-aqueous chemistry | Yes | SiPaste® C201HF |
| NC | Printing | Best-in-class transfer efficiency and stencil life Best all-around fine feature paste | DI water + saponifier or semi-aqueous chemistry | Yes | SiPaste® C312HF |
| NC-ULR | Printing | No-clean, ultra-low residue process that is compatible with post-reflow underfill | No-clean | Yes | SiPaste® SMQ77 |
| WS | Jetting | For dot jetting of 300 μm diameter and above, and fine-line dispensing for metallid-attach | Warm DI water | Yes | PicoShot® WS-5M |
| NC | Jetting | For dot jetting of 300 μm diameter and above, and fine-line dispensing for metallid-attach | Solvent- or aqueous-based chemistry or no-clean | Yes | PicoShot® NC-5M PicoShot® NC-6M |
| NC | Jetting | For dot jetting down to 80 μm diameter and above, and fine-line dispensing for metallid-attach | Solvent- or aqueous-based chemistry or no-clean | Yes | Indium12.8HF |
Product Data Sheets
SiPaste®C312HF Solder Paste PDS 100100 R4.pdf
SiPaste® 3.2HF Pb-Free Water-Sol Solder Paste for SiP Designs PDS 99821 R1.pdf
SnPb PicoShot® NC-5M PDS 100016 R5.pdf
SAC305 PicoShot® WS-5M PDS 100307 R1.pdf
Related Applications
Fine Powder Pastes can be used in a variety of applications.
Related Markets
Indium Corporation’s Fine Powder Pastes are applicable for use in many markets.
Expert Support for Reliable Results
Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!
Looking for Safety Data Sheets?
Access everything you need — from technical specifications to application guidance — in one convenient location.
Your Success
is Our Goal
Optimize your processes with the latest materials, technology, and expert application support. It all starts by connecting with our team.