The solidus and liquidus of off-eutectic alloys differ, creating a molten range where the allow appears plastic or pasty. As gallium nitride (GaN) dies gain popularity in high-frequency, high-power, and high-reliability RF power amplifiers for 5G, as well as crucial military and aerospace wireless communications, soldering these dies presents significant challenges.
GaN dies have thick gold plating—10 times thicker than is standard—to prevent oxidation, which can alter the final joint composition post-reflow, deviating from the desired 80Au20Sn composition. Maintaining the eutectic composition of 80Au20Sn in the solder joint is crucial for leveraging the unique properties of the alloy, particularly its high joint strength. Lowering the gold content in the alloy allows the solder to absorb some of the gold from the plating, resulting in a final strong joint composition of the eutectic 80Au20Sn.
Powered by Indium Corporation
- Strong Solder Joints in Die-Attach Applications
- Superior Wetting and Voiding
- Adjustment of the Final Solder Joint Composition
Product Overview
Available Alloys
- 79Au21Sn
- 78Au22Sn
- 75Au25Sn
Geometry
Guidelines for preform geometry can be derived from the die size. Generally, 90-100% of the die size indicates the preform’s x and y dimensions. Our AuLTRA® 75 off-eutectic AuSn alloys have thickness capabilities down to 0.005″. As for thickness, our Off-Eutectic AuSn alloys have thickness capabilities down to 0.0005″. The most critical attribute for a die bonding application is flatness. Due to process constraints, fixturing can be challenging and time consuming. Allowing the die to float freely on the preform can be advantageous. If the preform is not flat, it can skew the die during reflow and lead to failure. Proper processing is key to preserving flatness.
Alloy Chemistry
AuSn has a sensitive eutectic phase, which can be altered by Au-rich metallizations. This can result in areas that do not wet or flow properly, creating a weak solder joint. Adjustments with off-eutectic AuSn alloy compositions can be made to accommodate these metallizations, resulting in joint characteristics that are optimized for high reliability and performance.
Packaging
Packaging in waffle trays is the primary method for many die-attach applications while tape & reel is another similar technique that can be used. Both methods are suitable for automated assembly and offer excellent protection during transit and storage. Die-attach preforms can come in various sizes, so flexibility in design is important. We have an extensive library of trays and tape available.
AuLTRA® Off-Eutectic Preforms
See our available alloy compositions below:
| Alloy | Temperature (Solidus) | Temperature (Liquidus) |
|---|---|---|
| Au75Sn25 – Indalloy®270 | 278°C | 332°C |
| Au78Sn22 – Indalloy®269 | 278°C | 301°C |
| Au79Sn21 – Indalloy®271 | 278°C | 289°C |
Related Applications
AuLTRA® 75 off-eutectic preforms are suitable for a variety of applications.
Related Markets
Indium Corporation is a leading gold solder innovator for high-temperature, high-reliability, and critical applications such as die-attach and hermetic sealing in the following industries and markets:
Expert Support for Reliable Results
Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!
Looking for Safety Data Sheets?
Access everything you need — from technical specifications to application guidance — in one convenient location.
Your Success
is Our Goal
Optimize your processes with the latest materials, technology, and expert application support. It all starts by connecting with our team.