Products Solder Spheres

Specialty Solder Spheres

Indium Corporation is a small- to mid-volume supplier of specialty solder spheres. We offer a very wide variety of alloys and size range capabilities from around 0.004″ (100 μm) to 0.063″ (1.6 mm), depending on the alloy. Melting points range from below 90°C to over 700°C.

Powered by Indium Corporation

  • Low-Oxide Sphere
  • Tight Diameter Tolerance Control
  • Tight Alloy Composition Control
Microscopic view of uniform, spherical particles arranged on a dark background.

Features and Benefits

Specialty solder spheres are used in a variety of market segments, including medical, transportation and automotive, military and aerospace, high-end mobile, and computing. Clean manufacturing and processing ensure low-oxide levels with no organic contamination. All spheres are manufactured in IATF-16949 certified facilities.

  • Accurate diameters
  • Capable of supplying quantities from 1 sphere to > 20 million per month
  • Clean manufacturing and processing ensures low-oxide levels with no organic contamination
  • Whiteroom finishing and packaging ensures continuity of cleanliness
  • Pure metals ensure high-quality finished spheres
  • Manufactured in IATF-16949 certified facilities

Pb-Free Alloys

AlloyIndalloy® #Melting Point
Solidus (°C
)
Melting Point
Liquidus (°C)
Min
(in)*
Max
(in)*
Min
(µm)*
Max
(µm)*
In50Sn11181250.0040.030102762
In48Sn (In/Sn eutectic)1E1180.0040.035102889
Bi42Sn (Bi/Sn eutectic)2811380.0080.1092032,769
Bi42Sn1Ag2821391400.0080.030203762
99.99In (“Pure Indium”)41570.0040.0501021,270
Sn20In2.8Ag (Pb-free “Sn63”)2271751870.0040.030102762
Sn3.0Ag0.5Cu (SAC305)2562172200.0040.0651021,651
Sn4.0Ag0.5Cu (SAC405)25622172250.0040.035102889
Sn4Ag1212212280.0040.021102533
Sn5Ag1322212400.0040.032102800
80Au20Sn (Au/Sn eutectic)1822800.0040.039102991

*Approximate Manufacturable Diameter Range

Pb-Containing Alloys

AlloyIndalloy® #Melting Point
Solidus (°C
)
Melting Point
Liquidus (°C)
Min
(in)*
Max
(in)*
Min
(µm)*
Max
(µm)*
Sn46Pb8Bi2401601730.0100.030254762
Sn36Pb2Ag (Sn62)Sn621791810.0040.030102762
Sn37Pb (63Sn)1061830.0040.0501021,270
Pb25In1101831920.0040.027102686
Pb40In2061972310.0040.020102508
Pb10Sn1592753020.0040.0401021,016

*Approximate Manufacturable Diameter Range

Product Data Sheets

Specialty Solder Spheres PDS 97549 R10

Related Applications

Close-up of a square semiconductor chip with four subdivided sections on a green and black background.

Flip-Chip

A crucial technique in advanced semiconductor packaging.

SiP & Heterogeneous Integration Assembly (HIA)

SiP and Heterogeneous Integration Assembly (HIA)

System-in-package (SiP) and heterogeneous integration solutions

Two green microprocessor chips with one showing a grid of pins and the other displaying a central metallic square on a dark surface.

Ball-Attach

Including both water-wash and no-clean ball-attach fluxes

A close-up of a computer microchip with a metallic surface and visible internal components, showcasing advanced 2.5D packaging technology.

2.5D and 3D Packaging

Techniques to incorporate multiple dies in a…

Microchips on a printed circuit board

PCB Assembly

Proven and cutting-edge materials for PCB assembly…

Close-up of several industrial needles with a green blurred background.

Rework

Our rework solutions include solder wire, TACflux,…

Related Markets

Do you have technical questions or sales inquiries? Our dedicated team is here to help. “From One Engineer to Another®” isn’t just our motto—it’s our commitment to delivering exceptional service. We’re ready when you are. Let’s connect!

This image has an empty alt attribute; its file name is scientist-with-microscope.png

Looking for Safety Data Sheets?

Access everything you need — from technical specifications to application guidance — in one convenient location.