Indium Corporation’s Heat-Spring Thermal Interface Material Enhances Device Performance

Indium Corporation announces a soft metal alloy thermal interface material (SMA TIM) that offers high and uniform thermal resistance at lower applied stresses in compressed interfaces.

The company’s patented Heat-Spring® SMA TIM reduces thermal resistance and enhances cooling by utilizing two key properties of indium metal: superior thermal conductivity and malleability. Unlike standard thermal interface materials, Heat-Spring offers an extremely long service life as it does not pump out under power cycling, nor does it bake out over time. This combination of high conductance, high surface contact area (due to superior conformance), and low degradation over time produces a superior thermal interface and assures optimized long-term device performance.

Heat-Spring’s high and uniform thermal conductivity is enhanced further when placed under compression (35 to 100 psi).

Learn more at indiumstg.wpenginepowered.com/heat-spring or by contacting the company at [email protected].

Indium Corporation è uno dei principali produttori e fornitori di materiali per i mercati globali dell'elettronica, dei semiconduttori, dei film sottili, della gestione termica e del solare. I prodotti includono saldature e flussanti, brasature, materiali per interfacce termiche, bersagli per sputtering, metalli e composti inorganici di indio, gallio, germanio e stagno e NanoFoil®. Fondata nel 1934, Indium dispone di un'assistenza tecnica globale e di stabilimenti situati in Cina, Malesia, Singapore, Corea del Sud, Regno Unito e Stati Uniti.

Per ulteriori informazioni su Indium Corporation, visitate il sitoindiumstg.wpenginepowered.como inviate un’e-mailall’indirizzo [email protected]. Potete inoltre seguire i nostri esperti, From One Engineer ToAnother®(#FOETA), suwww.facebook.com/indiumo su@IndiumCorp.