Indium Corporation has announced a new jetting solder paste in its line of PicoShot products. PicoShot WS-5M is designed for customers needing an SnPb solder paste for their Mycronic MY-series jet printers.
PicoShot WS-5M is a water-soluble, halogen-free paste developed as a result of a close, collaborative relationship with Mycronic for their MY 600/700 jetting systems. This product has been beta-tested at customer sites, showing proven performance on customer lines.
PicoShot WS-5M has been extensively tested to provide exceptional jetting performance. It delivers:
- Smallest dot volume among pastes in its class: 6.5nl/dot, 350m diameter
- Präzisionsablage (x,y-Ausrichtung)
- Long usage (syringe life) >8 hours
- Minimal statellites
PicoShot WS-5M is a water-soluble, halogen-free solder paste approved after joint Indium/Mycronic technical development with Mycronic’s MY 600/700 jetting systems. PicoShot can be used in applications, such as jetting into cavities and uneven/warped substrates, high-mix/low-volume stencil replacement, CSP/microBGA solder attach, military and aerospace jetting applications, system-in-package (SiP), camera module assembly where an overmolding step is required, and shield-attach and secondary processing.
Utilizing a Type 5 solder powder and an SnPb alloy, this material is inherently chemically compatible with Indium Corporation’s Indium6.6HF-HD Solder Paste. PicoShot WS-5M’s unique oxidation barrier promotes complete powder coalescence during reflow to eliminate graping and similar reflow issues.
PicoShot WS-5M jetting solder paste is the second material to come out of Indium Corporation’s new partnership with Mycronic, a global leader in dispensing and jet printing equipment.
To learn more about Indium Corporation’s jetting pastes, visit https://www.indium.com/products/solders/solder-paste/#jetting-and-microdispensing.
Über Indium Corporation
Indium Corporation ist ein führender Materialveredler, -schmelzer, -hersteller und -lieferant für die weltweiten Elektronik-, Halbleiter-, Dünnschicht- und Wärmemanagementmärkte. Zu den Produkten gehören Lote und Flussmittel, Hartlote, Materialien für thermische Schnittstellen, Sputtertargets, Metalle und anorganische Verbindungen aus Indium, Gallium, Germanium und Zinn sowie NanoFoil. Das 1934 gegründete Unternehmen verfügt über einen weltweiten technischen Support und Fabriken in China, Deutschland, Indien, Malaysia, Singapur, Südkorea, dem Vereinigten Königreich und den Vereinigten Staaten.