Indium Corporation has released IndiOx™ (In2O3) for use in the manufacture of ITO sputtering targets for thin-film coating. IndiOx™ (In2O3) is a stable ceramic-like material that is insoluble in water and volatizes at 850°C.
When doped with tin oxide, IndiOx™ forms ITO, the material of choice to form transparent conductive oxide (TCO) layers in flat-panel displays and touch sensors for mobile devices. The ITO layer is deposited onto glass from a sputtering target that is manufactured from the ITO powder by sintering.
Other uses for IndiOx™ include glass coloring, gassing suppression in alkaline batteries, and as an anti-arcing additive in high current electrical switches and contactors.
IndiOx™ is available in three powder types:
- Type A – Crystalline: particle size distribution D10–D90 ranges from 0.8–38μm.
- Type B – Fine: particle size distribution D10–D90 ranges from 0.5–6μm.
- Type T – Target Grade: particle size distribution D10–D90 ranges from 0.1–7.5μm. The primary particle size is about 100nm.
For more information about Indium Corporation’s suite of compound materials, visit indiumstg.wpenginepowered.com/indiox.
Indium Corporation es uno de los principales fabricantes y proveedores de materiales para los mercados mundiales de la electrónica, los semiconductores, las películas finas y la gestión térmica. Sus productos incluyen soldaduras y fundentes, soldaduras fuertes, materiales de interfaz térmica, cátodos para sputtering, metales y compuestos inorgánicos de indio, galio, germanio y estaño, y NanoFoil®. Fundada en 1934, la empresa cuenta con asistencia técnica mundial y fábricas en China, India, Malasia, Singapur, Corea del Sur, Reino Unido y Estados Unidos.