Ir al contenido

Indium Corporation to Introduce Indium Oxide Powder at SVC TechCon 2018

Indium Corporation will introduce its new Indium Oxide High BET powder designed to support emerging applications of the display industry at SVC TechCon from May 5-10 in Orlando, Florida, USA.

Indium Corporation’s Indium Oxide High BET powder is designed for use in both display electrodes and thin-film oxide transistors as part of the transparent conductive oxide (TCO) film stack.

Indium Oxide High BET powder offers:

  • BET range from 13–17m2/g
  • Higher than 4N5 purity
  • Primary particle size between 50–100nm

This material supports the evolving needs of sputtering target production lines that need flexibility and the ability to scale in today’s fast-changing environment.

Indium Corporation’s reclaim capability includes a fully integrated manufacturing reclaim loop that provides a fast return-to-process time for our customers to lower inventory costs.

Visit us at booth #417 or find more information about our Indium Oxide products at https://www.indium.com/inorganic-compounds/indium-compounds/indium-oxide.

Para obtener más información sobre Indium Corporation, visitaindiumstg.wpenginepowered.como envía un correo electrónicoa [email protected]. También puedes seguir a nuestros expertos, From One Engineer ToAnother®(#FOETA), enwww.facebook.com/indiumo en@IndiumCorp.