Indium Corporation to Present at International Microwave Symposium

One of the most highly demanded applications for 80Au/20Sn is semiconductor laser die-attach due to recent advancements that have made lasers an economical option for a multitude of new products. However, a key challenge with semiconductor lasers is thermal management, as these devices generate a significant amount of heat. Indium Corporation Product Specialist Jenny Gallery will present on how to manage heat with AuSn preforms at the International Microwave Symposium, Denver, Colo., June 1924.

One method for facilitating thermal transfer from the die to the substrate is to reduce the bondline thickness through the use of thinner 80Au/20Sn preforms. By using a thinner preform in the bondline, the heat is transferred away from the die more quickly, increasing the longevity and potential of the die. In The Effect of Semiconductor Laser Thermal Transfer in Relation to AuSn Preform Thickness, Gallery will examine the impact of AuSn preform thickness on thermal transfer by examining voiding percentages on several 80Au/20Sn preforms ranging from 0.002 to 0.00035 thick. 

Gallery is a product specialist for the high-temperature business (gold and braze products) at Indium Corporation. She is responsible for researching and analyzing customer and market data, and she serves as a resource to the companys current and prospective customers, field sales, and internal departments. She provides product and process support for solder preforms, wire, ribbon, and paste, and she helps to facilitate relationships and new business development. Gallery earned her bachelors degree in chemistry at the University of Albany, N.Y., U.S. 

Acerca de Indium Corporation

Indium Corporation es un importante refinador, fundidor, fabricante y proveedor de materiales para los mercados mundiales de la electrónica, los semiconductores, las películas finas y la gestión térmica. Sus productos incluyen soldaduras y fundentes; soldaduras fuertes; materiales de interfaz térmica; cátodos para sputtering; metales y compuestos inorgánicos de indio, galio, germanio y estaño; y NanoFoil. Fundada en 1934, la empresa cuenta con asistencia técnica mundial y fábricas en China, Alemania, India, Malasia, Singapur, Corea del Sur, Reino Unido y Estados Unidos.

Para obtener más información sobre Indium Corporation, visitaindiumstg.wpenginepowered.como envía un correo electrónico aJingya Huang. También puedes seguir a nuestros expertos, «From One Engineer To Another» (, #FOETA), enwww.linkedin.com/company/indium-corporation/o en@IndiumCorp.

Acerca del Simposio Internacional de Microondas

For 70 years, IMS has brought together a unique mix of international RF and microwave experts presenting the latest research and showcasing the new products and services. IMS includes education and networking opportunities as well as an exhibition. Learn more at ims-ieee.org.