Indium Corporation ofrece una solución única para aplicaciones de estaño (Sn) metálico de gran pureza

Indium Corporation delivers a single-source solution, from mine to packaging, for high-purity tin materials. The company offers tin in a number of physical forms and purity levels of up to 5N or 99.999%-pure.

With a melting point of 505.08 K (231.93°C or 449.47°F) as well as its corrosion-resistant nature, tin is becoming increasingly popular for a number of new and innovative applications, including aerospace and semiconductor.

Indium Corporation delivers tin in grades of 99% (2N) through 99.999%-pure (5N) in a number of physical shapes and geometry, including:

  • Lingote
  • Disparo
  • Polvo
  • Fabricaciones del cliente (esferas, alambres, tubos, etc.)

For more information, visit indiumstg.wpenginepowered.com/tin or contact Donna Vareha-Walsh, Director Metals Business Unit, at [email protected].

Indium Corporation es uno de los principales fabricantes y proveedores de materiales para los mercados mundiales de la electrónica, los semiconductores, las películas finas y la gestión térmica. Sus productos incluyen soldaduras y fundentes; soldaduras fuertes; materiales de interfaz térmica; cátodos para sputtering; metales y compuestos inorgánicos de indio, galio, germanio y estaño; y NanoFoil®. Fundada en 1934, Indium cuenta con asistencia técnica mundial y fábricas en China, Malasia, Singapur, Corea del Sur, Reino Unido y Estados Unidos.

Para obtener más información sobre Indium Corporation, visitaindiumstg.wpenginepowered.como envía un correo electrónicoa [email protected]. También puedes seguir a nuestros expertos, From One Engineer ToAnother®(#FOETA), enwww.facebook.com/indiumo en@IndiumCorp.