Indium Corporation has released Indium11.8HF-SPR (T5-MC) Solder Paste a new air and nitrogen reflow, no-clean, Pb-free solder paste designed to meet the fine feature printing requirements of mobile manufacturers.
Indium11.8HF-SPR specifically addresses the move toward type 5 powder. This new solder paste delivers unprecedented stencil print transfer efficiency on the broadest range of processes, while maintaining industry-leading reflow performance.
Avantages de l'Indium11.8HF-SPR :
- Sans halogène selon la méthode d'essai IEC 61249-2-21 EN14582
- High-transfer efficiency through small apertures ( 0.66AR)
- Long stencil life (>12 hours)
- Eliminates hot and cold slump to inhibit bridging and solder beading defects
- Avoids the potential for HIP and graping defects with a unique oxidation barrier
Indium Corporation is a premier materials manufacturer and supplier to the global electronics, semiconductor, thin-film, and thermal management markets. Products include solders and fluxes; brazes; thermal interface materials; sputtering targets; indium, gallium, germanium, and tin metals and inorganic compounds; and NanoFoil. Founded in 1934, Indium has global technical support and factories located in China, Malaysia, Singapore, South Korea, the United Kingdom, and the USA.
For more information about Indium Corporation, visit indiumstg.wpenginepowered.com or email [email protected]. You can also follow our experts, From One Engineer To Another (#FOETA), at www.facebook.com/indium or @IndiumCorp.